Magnesium AZ31B-H24 vs. SLA Resin Elastic 50A Compare Magnesium AZ31B-H24 vs. SLA Resin Elastic 50A strength, stiffness, weight and thermal properties.
Change either side
Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless 304 Stainless 316 Stainless 303 Stainless 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall Magnesium AZ31B-H24 Wrought Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless 304 Stainless 316 Stainless 303 Stainless 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall SLA Resin Elastic 50A 3D printed (SLA resin) Try it on a partA bracket to run stress or thermal on, free in your browser Open in LessCAD Open in LessCAD Mechanical Yield strength 220 MPa source typical, H24, 0.5-6 mm, 0.2 % proof stress not given (tensile used) Ultimate tensile strength 290 MPa source typical, H24, 0.5-6 mm 3.4 MPa source typical Elongation at break 13 % source typical, H24, 0.5-6 mm, gauge 5.65√A 160 % source typical Young's modulus (stiffness) 44.8 GPa source typical (handbook physical constant) not sourced Density 1,769 kg/m³ source nominal 1,010 kg/m³ source typical Strength to weight 124 kN·m/kg 36.9x higher 3.37 kN·m/kg Stiffness to weight 25.3 MN·m/kg not sourced Poisson's ratio 0.35 source typical (handbook physical constant) not sourced Shear modulus 16.6 GPa not sourced Bulk modulus 49.8 GPa not sourced Speed of sound 5,032 m/s not sourced Thermal Thermal conductivity 76.9 W/m·K source typical (temper/temperature not stated) not sourced Thermal expansion 26.8 µm/m·K source typical (temperature range not stated) not sourced 100 mm part over a 50 °C swing 134 µm growth not sourced Specific heat 1,040 J/kg·K source typical not sourced Heats up and cools (diffusivity) 41.8 mm²/s not sourced Thermal shock resistance 9,159 W/m not sourced Glass transition not sourced -34.5 °C source DMA Max service temperature 149 °C source stated application limit not sourced Values for AZ31B-H24 sheet 0.016-0.062 in., MIL-HDBK-5J Table 4.2.1.0(b) (AMS 4377); strengths are S-basis MINIMUMS Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions Is Magnesium AZ31B-H24 stronger than SLA Resin Elastic 50A? Magnesium AZ31B-H24 is stronger: its yield strength is 220 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (64.7x).
Which is lighter, Magnesium AZ31B-H24 or SLA Resin Elastic 50A? SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 1,769 kg/m³ for Magnesium AZ31B-H24.
Which is lighter for the same job, Magnesium AZ31B-H24 or SLA Resin Elastic 50A? For the same stiffness or strength: Magnesium AZ31B-H24 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be Magnesium AZ31B-H24 SLA Resin Elastic 50A Strong rod or tie lighter 36.9x heavier Strong beam lighter 9.2x heavier Strong panel or plate lighter 4.59x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Among 59 materials 1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Aluminum Steel Iron Titanium Steel AISI 1018 Stainless 304 Stainless 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless 303 Stainless 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Magnesium AZ31B-H24 Stiffness against density 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Rubber Aluminum Steel Iron Titanium Steel AISI 1018 Stainless 304 Stainless 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless 303 Stainless 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick Magnesium AZ31B-H24 SLA Resin Elastic 50A Strength against density