| Mechanical | ||
| Yield strength | 220MPasourcetypical, H24, 0.5-6 mm, 0.2 % proof stress | 885MPasourcetypical, plate (>0.187 in), annealed, 0.2% offset |
| Ultimate tensile strength | 290MPasourcetypical, H24, 0.5-6 mm | 940MPasourcetypical, plate, annealed |
| Elongation at break | 13%sourcetypical, H24, 0.5-6 mm, gauge 5.65√A | 16%sourcetypical, in 2 in., plate annealed |
| Young's modulus (stiffness) | 44.8GPasourcetypical (handbook physical constant) | 107–122GPasourcetypical range, 20 °C |
| Density | 1,769kg/m³sourcenominal2.5x lighter | 4,430kg/m³sourcenominal |
| Strength to weight | 124kN·m/kg | 200kN·m/kg1.61x higher |
| Stiffness to weight | 25.3MN·m/kg | 25.8MN·m/kg2% higher |
| Poisson's ratio | 0.35sourcetypical (handbook physical constant) | 0.342sourcemean of TIMET measurements |
| Shear modulus | 16.6GPa | 42.7GPa2.57x stiffer in shear |
| Bulk modulus | 49.8GPa | 121GPa |
| Speed of sound | 5,032m/s | 5,084m/s |
| Thermal | ||
| Thermal conductivity | 76.9W/m·Ksourcetypical (temper/temperature not stated) | 6.6W/m·Ksourcetypical, 20 °C, mill annealed |
| Thermal expansion | 26.8µm/m·Ksourcetypical (temperature range not stated) | 9µm/m·Ksourcetypical, mean 0-100 °C |
| 100 mm part over a 50 °C swing | 134µm growth | 45µm growth2.98x less |
| Specific heat | 1,040J/kg·Ksourcetypical | 580J/kg·Ksourcetypical, 20 °C |
| Heats up and cools (diffusivity) | 41.8mm²/s16.3x faster | 2.57mm²/s |
| Thermal shock resistance | 9,159W/m2.46x more resistant | 3,730W/m |
| Melting point | not sourced | 1,630–1,650°Csourcemelting range |
| Max service temperature | 149°Csourcestated application limit | 400°Csourceupper recommended use temperature |
| Values for | AZ31B-H24 sheet 0.016-0.062 in., MIL-HDBK-5J Table 4.2.1.0(b) (AMS 4377); strengths are S-basis MINIMUMS | TIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties |
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Is Magnesium AZ31B-H24 stronger than Titanium?
Titanium is stronger: its yield strength is 885 MPa against 220 MPa for Magnesium AZ31B-H24 (4.02x).
Which is lighter, Magnesium AZ31B-H24 or Titanium?
Magnesium AZ31B-H24 is lighter: 1,769 kg/m³ against 4,430 kg/m³ for Titanium.
Which is stiffer, Magnesium AZ31B-H24 or Titanium?
Titanium is stiffer: Young's modulus 115 GPa against 44.8 GPa for Magnesium AZ31B-H24, so the same part in Titanium deflects less under the same load.
Which is lighter for the same job, Magnesium AZ31B-H24 or Titanium?
For the same stiffness or strength: Magnesium AZ31B-H24 is lighter for a stiff beam (bending), stiff panel or plate, strong panel or plate; Titanium is lighter for a stiff rod or tie (tension), strong rod or tie.
| Part that must be | Magnesium AZ31B-H24 | Titanium |
|---|---|---|
| Stiff rod or tie (tension) | 2% heavier | lighter |
| Stiff beam (bending) | lighter | 1.57x heavier |
| Stiff panel or plate | lighter | 1.83x heavier |
| Strong rod or tie | 1.61x heavier | lighter |
| Strong beam | about equal | about equal |
| Strong panel or plate | lighter | 25% heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which conducts heat better, Magnesium AZ31B-H24 or Titanium?
Magnesium AZ31B-H24 conducts heat better: 76.9 W/m·K against 6.6 W/m·K for Titanium.
Which expands less with temperature?
Titanium expands less: 9 µm/m·K against 26.8 µm/m·K for Magnesium AZ31B-H24.