SLS PA12 Nylon vs. Steel

Compare SLS PA12 Nylon vs. Steel strength, stiffness, weight and thermal properties.

Change either side
SLS PA12 Nylon3D printed (SLS)
SteelWrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)385MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISC
Ultimate tensile strength48MPasourcetypical505MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)
Elongation at break18%sourcetypicalnot sourced
Young's modulus (stiffness)1.65GPasourcetypical200GPasourcedesign value (AISC 360-16)
Density930kg/m³sourcetypical7,850kg/m³sourcenominal (constructional data)
Strength to weight51.6kN·m/kg5% higher49kN·m/kg
Stiffness to weight1.77MN·m/kg25.5MN·m/kg14.4x higher
Poisson's rationot sourced0.3sourcedesign value (AISC 360-16 Commentary)
Shear modulusnot sourced76.9GPa
Bulk modulusnot sourced167GPa
Speed of sound1,332m/s5,048m/s
Thermal
Thermal conductivitynot sourced48W/m·Ksourcenominal at 20 °C
Thermal expansionnot sourced12µm/m·Ksourcenominal (constructional data, no temperature range stated)
100 mm part over a 50 °C swingnot sourced60µm growth
Specific heatnot sourced460–480J/kg·Ksourcebase material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Heats up and cools (diffusivity)not sourced13mm²/s
Thermal shock resistancenot sourced5,390W/m
Melting point176°Csourcetypicalnot sourced
Max service temperature64°CsourceHDT 1.8 MPa, X orientationnot sourced
Values forEOS PA 2200 (PA12) Material Data Sheet, process parameter 'Balance' at 120 µm layer thickness, X orientation, dry (conditioned values not given). Live MDS status 04.10.2026, last changed 10.09.2026; PDF via ?topdf=... link on the same page.Generic structural steel, cited as ASTM A992 (the current US structural grade): ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLS PA12 Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is SLS PA12 Nylon stronger than Steel?

Steel is stronger: its yield strength is 385 MPa against tensile strength 48 MPa for SLS PA12 Nylon (8.02x).

Which is lighter, SLS PA12 Nylon or Steel?

SLS PA12 Nylon is lighter: 930 kg/m³ against 7,850 kg/m³ for Steel.

Which is stiffer, SLS PA12 Nylon or Steel?

Steel is stiffer: Young's modulus 200 GPa against 1.65 GPa for SLS PA12 Nylon, so the same part in Steel deflects less under the same load.

Which is lighter for the same job, SLS PA12 Nylon or Steel?

For the same stiffness or strength: SLS PA12 Nylon is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Steel is lighter for a stiff rod or tie (tension), stiff beam (bending).

Part that must beSLS PA12 NylonSteel
Stiff rod or tie (tension)14.4x heavierlighter
Stiff beam (bending)30% heavierlighter
Stiff panel or platelighter1.71x heavier
Strong rod or tielighter5% heavier
Strong beamlighter2.11x heavier
Strong panel or platelighter2.98x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000DMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelSLS PA12 NylonSteel
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ADMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickSLS PA12 NylonSteel
Strength against density

Related comparisons