Materials / Compare

Plastic PETG vs. Plywood

Compare Plastic PETG vs. Plywood strength, stiffness, weight and thermal properties.

Change either side
Plastic PETG3D printed (FDM)
PlywoodNatural
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength46.2MPasourcetypicalnot given (tensile used)
Ultimate tensile strength46.2MPasourcetypical, peak stress (= stress at yield)41.4MPasourcemodulus of rupture (no direct tensile value)
Flexural strength78.9MPasourcetypical41.4MPasourcestatic bending MOR (Douglas-fir); range 33.72-42.61 across species
Elongation at break7.6%sourcetypicalnot sourced
Young's modulus (stiffness)1.94GPasourcetypical7.45GPasourcestatic bending MOE of the panel (Douglas-fir); range 6.96-8.55 across species
Density1,270kg/m³sourcetypicalnot sourced
Strength to weight36.4kN·m/kgnot sourced
Stiffness to weight1.53MN·m/kgnot sourced
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,236m/snot sourced
Thermal
Thermal conductivity0.21W/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical0.12W/m·KsourceAPA-recommended design value (Douglas-fir plywood), as reported by FPL/ORNL
Thermal expansion51µm/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical3.1–4.5µm/m·Ksourcebase material: solid wood parallel to grain, ovendry, range across species
100 mm part over a 50 °C swing255µm growth19µm growth13.4x less
Specific heat1,300J/kg·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)1,700J/kg·Ksourcebase material: solid wood (all species), 12% MC, 27 C
Heats up and cools (diffusivity)0.127mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Glass transition77.4°Csourcetypicalnot sourced
Max service temperature76.2°CsourceHDT 0.455 MPa (printed specimens)not sourced
Values forUltimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022.Douglas-fir plywood sheathing (construction plywood per PS 1), static bending properties from USDA FPL Wood Handbook FPL-GTR-282 Ch. 12 Table 12-2 (Biblis 2000)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic PETG stronger than Plywood?

Plastic PETG is stronger: its yield strength is 46.2 MPa against tensile strength 41.4 MPa for Plywood (12%).

Which is stiffer, Plastic PETG or Plywood?

Plywood is stiffer: Young's modulus 7.45 GPa against 1.94 GPa for Plastic PETG, so the same part in Plywood deflects less under the same load.

Which conducts heat better, Plastic PETG or Plywood?

Plastic PETG conducts heat better: 0.21 W/m·K against 0.12 W/m·K for Plywood.

Which expands less with temperature?

Plywood expands less: 3.8 µm/m·K against 51 µm/m·K for Plastic PETG.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PETG
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PETG
Strength against density

Related comparisons