Materials / Compare
Plastic ABS (bulk/injection) vs. Steel AISI 1018
Compare Plastic ABS (bulk/injection) vs. Steel AISI 1018 strength, stiffness, weight and thermal properties.
| Mechanical | Plastic ABS (bulk/injection) | Steel AISI 1018 |
|---|---|---|
| Yield strength | 45MPa1 | producer-stated372MPa28.27x stronger |
| Ultimate tensile strength | not stated (yield given) | producer-stated441MPa2 |
| Flexural strength | 65MPa1 | not sourced |
| Elongation at break | 10%1 | in 2 in15%21.5x more ductile |
| Young's modulus (stiffness) | 2.3GPa1 | base material200GPa3 |
| Density | 1,040kg/m³1 | base material7,861kg/m³3 |
| Strength to weight | 43.3kN·m/kg | 47.3kN·m/kg9% higher |
| Stiffness to weight | 2.21MN·m/kg | 25.4MN·m/kg11.5x higher |
| Poisson's ratio | 0.394 | base material0.323 |
| Shear modulus | 0.827GPa | 75.7GPa91.5x stiffer in shear |
| Bulk modulus | 3.48GPa | 185GPa53.1x higher |
| Speed of sound | 1,487m/s | 5,043m/s3.39x faster |
| Thermal | Plastic ABS (bulk/injection) | Steel AISI 1018 |
|---|---|---|
| Thermal conductivity | 0.17W/m·K1 | base material51.9W/m·K3 |
| Thermal expansion | range80–110µm/m·K1 | base material12µm/m·K5 |
| 100 mm part over a 50 °C swing | 475µm growth | 60µm growth7.92x less |
| Specific heat | not sourced | base material486J/kg·K3 |
| Heats up and cools (diffusivity) | not sourced | 13.6mm²/s |
| Thermal shock resistance | 21.4W/m | 5,473W/m256x more resistant |
| Max service temperature | HDT 1.8 MPa94°C1 | not sourced |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources5 documents: INEOS Styrolution, Niagara LaSalle, U.S. Department of Defense, Covestro, Ovako
- Plastic ABS (bulk/injection)
- INEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)
- Steel AISI 1018
- AISI 1018 cold drawn bar (Niagara LaSalle, cold-finished bar producer)
- 1Terluran GP-22 (ABS) Product Data SheetINEOS StyrolutionPlastic ABS (bulk/injection) · Yield strength: typical, tensile stress at yield 23 °CPlastic ABS (bulk/injection) · Flexural strength: typical, 23 °CPlastic ABS (bulk/injection) · Elongation at break: nominal strain at break, 23 °CPlastic ABS (bulk/injection) · Young's modulus (stiffness): typicalPlastic ABS (bulk/injection) · Density: typicalPlastic ABS (bulk/injection) · Thermal conductivity: typicalPlastic ABS (bulk/injection) · Thermal expansion: rangePlastic ABS (bulk/injection) · Max service temperature: HDT 1.8 MPa (annealed 4 h/80 °C)
- 21018 PropertiesNiagara LaSallearchived copySteel AISI 1018 · Yield strength: producer-stated, cold drawnSteel AISI 1018 · Ultimate tensile strength: producer-stated, cold drawnSteel AISI 1018 · Elongation at break: in 2 in (50.8 mm)
- 3MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 1018 · Young's modulus (stiffness): base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Density: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Poisson's ratio: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Thermal conductivity: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Specific heat: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
- 4Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic ABS (bulk/injection) · Poisson's ratio: typical, ABS family (Covestro Part and Mold Design guide, Table 3-1)
- 5S275JR Steel GradeOvakoSteel AISI 1018 · Thermal expansion: base material: unalloyed carbon steel, Ovako family table (S275JR, 'none alloyed structural steels', C <= 0.21%); mean 20-300 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic ABS (bulk/injection) stronger than Steel AISI 1018?
Steel AISI 1018 is stronger: its yield strength is 372 MPa against 45 MPa for Plastic ABS (bulk/injection) (8.27x).
Which is lighter, Plastic ABS (bulk/injection) or Steel AISI 1018?
Plastic ABS (bulk/injection) is lighter: 1,040 kg/m³ against 7,861 kg/m³ for Steel AISI 1018.
Which is stiffer, Plastic ABS (bulk/injection) or Steel AISI 1018?
Steel AISI 1018 is stiffer: Young's modulus 200 GPa against 2.3 GPa for Plastic ABS (bulk/injection), so the same part in Steel AISI 1018 deflects less under the same load.
Which is lighter for the same job, Plastic ABS (bulk/injection) or Steel AISI 1018?
For the same stiffness or strength: Plastic ABS (bulk/injection) is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel AISI 1018 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.
| Part that must be | Plastic ABS (bulk/injection) | Steel AISI 1018 |
|---|---|---|
| Stiff rod or tie (tension) | 11.5x heavier | lighter |
| Stiff beam (bending) | 23% heavier | lighter |
| Stiff panel or plate | lighter | 1.71x heavier |
| Strong rod or tie | 9% heavier | lighter |
| Strong beam | lighter | 1.85x heavier |
| Strong panel or plate | lighter | 2.63x heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic ABS (bulk/injection) or Steel AISI 1018?
Steel AISI 1018 stretches further before it breaks: 15% elongation at break against 10% for Plastic ABS (bulk/injection).
Thermal
Which conducts heat better, Plastic ABS (bulk/injection) or Steel AISI 1018?
Steel AISI 1018 conducts heat better: 51.9 W/m·K against 0.17 W/m·K for Plastic ABS (bulk/injection).
Which expands less with temperature?
Steel AISI 1018 expands less: 12 µm/m·K against 95 µm/m·K for Plastic ABS (bulk/injection).
Related comparisons
- Plastic ABS (bulk/injection) vs. FDM ASA
- Plastic ABS (bulk/injection) vs. FDM Polycarbonate
- Plastic ABS (bulk/injection) vs. Plastic ABS
- Plastic ABS (bulk/injection) vs. Plastic PETG
- Steel AISI 1018 vs. Steel
- Steel AISI 1018 vs. Steel A992
- Steel AISI 1018 vs. Stainless Steel 303
- Steel AISI 1018 vs. Stainless Steel 316