Materials / Compare

Plastic ABS (bulk/injection) vs. Titanium

Compare Plastic ABS (bulk/injection) vs. Titanium strength, stiffness, weight and thermal properties.

Plastic ABS (bulk/injection)Bulk polymer (molded or machined)
TitaniumWrought
MechanicalPlastic ABS (bulk/injection)Titanium
Yield strength45MPa1885MPa219.7x stronger
Ultimate tensile strengthnot stated (yield given)940MPa2
Flexural strength65MPa1not sourced
Elongation at break10%116%21.6x more ductile
Young's modulus (stiffness)2.3GPa1107–122GPa3
Density1,040kg/m³14.26x lighter4,430kg/m³2
Strength to weight43.3kN·m/kg200kN·m/kg4.62x higher
Stiffness to weight2.21MN·m/kg25.8MN·m/kg11.7x higher
Poisson's ratio0.3940.3422
Shear modulus0.827GPa42.7GPa51.6x stiffer in shear
Bulk modulus3.48GPa121GPa34.7x higher
Speed of sound1,487m/s5,084m/s3.42x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Titanium
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Titanium
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic ABS (bulk/injection)Titanium
Thermal conductivity0.17W/m·K16.6W/m·K338.8x more heat through a fin
Thermal expansionrange80–110µm/m·K19µm/m·K3
100 mm part over a 50 °C swing475µm growth45µm growth10.6x less
Specific heatnot sourced580J/kg·K3
Heats up and cools (diffusivity)not sourced2.57mm²/s
Thermal shock resistance21.4W/m3,730W/m175x more resistant
Melting pointnot sourcedmelting range1,630–1,650°C2
Max service temperatureHDT 1.8 MPa94°C1400°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Titanium
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABS (bulk/injection)Titanium
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: INEOS Styrolution, TIMET, Covestro
Plastic ABS (bulk/injection)
INEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)
Titanium
TIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties
  1. 1
    Terluran GP-22 (ABS) Product Data SheetINEOS StyrolutionPlastic ABS (bulk/injection) · Yield strength: typical, tensile stress at yield 23 °CPlastic ABS (bulk/injection) · Flexural strength: typical, 23 °CPlastic ABS (bulk/injection) · Elongation at break: nominal strain at break, 23 °CPlastic ABS (bulk/injection) · Young's modulus (stiffness): typicalPlastic ABS (bulk/injection) · Density: typicalPlastic ABS (bulk/injection) · Thermal conductivity: typicalPlastic ABS (bulk/injection) · Thermal expansion: rangePlastic ABS (bulk/injection) · Max service temperature: HDT 1.8 MPa (annealed 4 h/80 °C)
  2. 2
    TIMETAL 6-4 PropertiesTIMETarchived copyTitanium · Yield strength: typical, plate (>0.187 in), annealed, 0.2% offsetTitanium · Ultimate tensile strength: typical, plate, annealedTitanium · Elongation at break: typical, in 2 in., plate annealedTitanium · Density: nominalTitanium · Poisson's ratio: mean of TIMET measurementsTitanium · Melting point: melting rangeTitanium · Max service temperature: upper recommended use temperature
  3. 3
    TIMETAL 6-4 Data SheetTIMETarchived copyTitanium · Young's modulus (stiffness): typical range, 20 °CTitanium · Thermal conductivity: typical, 20 °C, mill annealedTitanium · Thermal expansion: typical, mean 0-100 °CTitanium · Specific heat: typical, 20 °C
  4. 4
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic ABS (bulk/injection) · Poisson's ratio: typical, ABS family (Covestro Part and Mold Design guide, Table 3-1)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Plastic ABS (bulk/injection) stronger than Titanium?

Titanium is stronger: its yield strength is 885 MPa against 45 MPa for Plastic ABS (bulk/injection) (19.7x).

Which is lighter, Plastic ABS (bulk/injection) or Titanium?

Plastic ABS (bulk/injection) is lighter: 1,040 kg/m³ against 4,430 kg/m³ for Titanium.

Which is stiffer, Plastic ABS (bulk/injection) or Titanium?

Titanium is stiffer: Young's modulus 115 GPa against 2.3 GPa for Plastic ABS (bulk/injection), so the same part in Titanium deflects less under the same load.

Which is lighter for the same job, Plastic ABS (bulk/injection) or Titanium?

For the same stiffness or strength: Plastic ABS (bulk/injection) is lighter for a stiff panel or plate; Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABS (bulk/injection)Titanium
Stiff rod or tie (tension)11.7x heavierlighter
Stiff beam (bending)1.66x heavierlighter
Stiff panel or platelighter16% heavier
Strong rod or tie4.62x heavierlighter
Strong beam1.71x heavierlighter
Strong panel or plate4% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic ABS (bulk/injection) or Titanium?

Titanium stretches further before it breaks: 16% elongation at break against 10% for Plastic ABS (bulk/injection).

Thermal

Which conducts heat better, Plastic ABS (bulk/injection) or Titanium?

Titanium conducts heat better: 6.6 W/m·K against 0.17 W/m·K for Plastic ABS (bulk/injection).

Which expands less with temperature?

Titanium expands less: 9 µm/m·K against 95 µm/m·K for Plastic ABS (bulk/injection).