Materials / Compare

Plastic PLA vs. Plastic TPU

Compare Plastic PLA vs. Plastic TPU strength, stiffness, weight and thermal properties.

Change either side
Plastic PLA3D printed (FDM)
Plastic TPU3D printed (FDM)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength52.5MPasourcetypicalnot given (tensile used)
Ultimate tensile strength52.5MPasourcetypical, peak stress (= stress at yield)23.7MPasourcetypical, stress at break
Flexural strength96.8MPasourcetypical23.6x stronger in bending4.1MPasourcetypical
Elongation at break7.8%sourcetypicalnot sourced
Young's modulus (stiffness)3.25GPasourcetypical48.5x stiffer0.067GPasourcetypical
Density1,240kg/m³sourcetypical1,220kg/m³sourcetypical
Strength to weight42.3kN·m/kg2.18x higher19.4kN·m/kg
Stiffness to weight2.62MN·m/kg47.7x higher0.0549MN·m/kg
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,619m/s234m/s
Thermal
Thermal conductivity0.13W/m·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °Cnot sourced
Thermal expansionnot sourcednot sourced
100 mm part over a 50 °C swingnot sourcednot sourced
Specific heat1,200J/kg·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °Cnot sourced
Heats up and cools (diffusivity)0.0874mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Melting point152°Csourcetypical217°Csourcetypical
Glass transition59.1°Csourcetypicalnot sourced
Max service temperature58.8°CsourceHDT 0.455 MPa (printed specimens)17% hotter50.3°CsourceHDT 0.455 MPa (printed specimens)
Values forUltimaker PLA, 3D-printed specimens, XY (flat) orientation; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS dated April 20, 2022.Ultimaker TPU 95A, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 29, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PLA and Plastic TPU are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic PLA stronger than Plastic TPU?

Plastic PLA is stronger: its yield strength is 52.5 MPa against tensile strength 23.7 MPa for Plastic TPU (2.22x).

Which is lighter, Plastic PLA or Plastic TPU?

Plastic TPU is lighter: 1,220 kg/m³ against 1,240 kg/m³ for Plastic PLA.

Which is stiffer, Plastic PLA or Plastic TPU?

Plastic PLA is stiffer: Young's modulus 3.25 GPa against 0.067 GPa for Plastic TPU, so the same part in Plastic PLA deflects less under the same load.

Which is lighter for the same job, Plastic PLA or Plastic TPU?

For the same stiffness or strength: Plastic PLA is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PLAPlastic TPU
Stiff rod or tie (tension)lighter47.7x heavier
Stiff beam (bending)lighter6.85x heavier
Stiff panel or platelighter3.59x heavier
Strong rod or tielighter2.18x heavier
Strong beamlighter1.67x heavier
Strong panel or platelighter46% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which handles higher temperatures, Plastic PLA or Plastic TPU?

Plastic PLA does: 58.8 °C against 50.3 °C for Plastic TPU, both HDT 0.455 MPa (printed specimens).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PETGPlastic ABSPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PLAPlastic TPU
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PETGPlastic ABSPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PLAPlastic TPU
Strength against density

Related comparisons