Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: UltiMaker, Outokumpu, Steel Construction Institute, NatureWorks, Carpenter Technology
Plastic PLA
Ultimaker PLA, 3D-printed specimens, XY (flat) orientation; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS dated April 20, 2022.
Stainless Steel 303
1.4305 / UNS S30300, Outokumpu typical values (hot rolled, solution annealed) from 'Steel Grades, Properties and Global Standards'; max service from Carpenter CarTech 303 datasheet
Steel Grades, Properties and Global StandardsOutokumpuarchived copyStainless Steel 303 · Yield strength: Outokumpu typical (product P = hot rolled plate, transverse)Stainless Steel 303 · Ultimate tensile strength: Outokumpu typicalStainless Steel 303 · Elongation at break: Outokumpu typical, A5Stainless Steel 303 · Young's modulus (stiffness): at RT (Table 12)Stainless Steel 303 · Density: at RTStainless Steel 303 · Thermal conductivity: at RTStainless Steel 303 · Thermal expansion: mean, 20–100 °CStainless Steel 303 · Specific heat: at RT
3
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 303 · Poisson's ratio: design value (structural stainless steels)
4
Engineering Properties of Ingeo BiopolymerNatureWorksarchived copyPlastic PLA · Thermal conductivity: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °CPlastic PLA · Specific heat: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C
5
Carpenter Stainless Type 303 Data SheetCarpenter Technologyarchived copyStainless Steel 303 · Max service temperature: continuous, scaling limit
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Plastic PLA is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Plastic PLA stronger than Stainless Steel 303?
Stainless Steel 303 is stronger: its yield strength is 275 MPa against 52.5 MPa for Plastic PLA (5.24x).
Which is lighter, Plastic PLA or Stainless Steel 303?
Plastic PLA is lighter: 1,240 kg/m³ against 7,900 kg/m³ for Stainless Steel 303.
Which is stiffer, Plastic PLA or Stainless Steel 303?
Stainless Steel 303 is stiffer: Young's modulus 200 GPa against 3.25 GPa for Plastic PLA, so the same part in Stainless Steel 303 deflects less under the same load.
Which is lighter for the same job, Plastic PLA or Stainless Steel 303?
For the same stiffness or strength: Plastic PLA is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 303 is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
Plastic PLA
Stainless Steel 303
Stiff rod or tie (tension)
9.66x heavier
lighter
Stiff beam (bending)
23% heavier
lighter
Stiff panel or plate
lighter
1.61x heavier
Strong rod or tie
lighter
22% heavier
Strong beam
lighter
2.11x heavier
Strong panel or plate
lighter
2.78x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PLA or Stainless Steel 303?
Stainless Steel 303 stretches further before it breaks: 35% elongation at break against 7.8% for Plastic PLA.
Thermal
Which conducts heat better, Plastic PLA or Stainless Steel 303?
Stainless Steel 303 conducts heat better: 15 W/m·K against 0.13 W/m·K for Plastic PLA.