Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 4340 · Young's modulus (stiffness): MIL-HDBK-5J design value (AISI 4340, quenched and tempered)Steel AISI 4340 · Poisson's ratio: MIL-HDBK-5J design value (AISI 4340, quenched and tempered)
4
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
5
Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic Polycarbonate stronger than Steel AISI 4340?
Steel AISI 4340 is stronger: its yield strength is 1,035 MPa against 65 MPa for Plastic Polycarbonate (15.9x).
Which is lighter, Plastic Polycarbonate or Steel AISI 4340?
Plastic Polycarbonate is lighter: 1,200 kg/m³ against 7,840 kg/m³ for Steel AISI 4340.
Which is stiffer, Plastic Polycarbonate or Steel AISI 4340?
Steel AISI 4340 is stiffer: Young's modulus 200 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Steel AISI 4340 deflects less under the same load.
Which is lighter for the same job, Plastic Polycarbonate or Steel AISI 4340?
For the same stiffness or strength: Plastic Polycarbonate is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel AISI 4340 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.
Part that must be
Plastic Polycarbonate
Steel AISI 4340
Stiff rod or tie (tension)
12.7x heavier
lighter
Stiff beam (bending)
40% heavier
lighter
Stiff panel or plate
lighter
50% heavier
Strong rod or tie
2.44x heavier
lighter
Strong beam
lighter
3% heavier
Strong panel or plate
lighter
1.64x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic Polycarbonate or Steel AISI 4340?
Plastic Polycarbonate stretches further before it breaks: 125% elongation at break against 18% for Steel AISI 4340.
Thermal
Which conducts heat better, Plastic Polycarbonate or Steel AISI 4340?
Steel AISI 4340 conducts heat better: 37.5 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.
Which expands less with temperature?
Steel AISI 4340 expands less: 11.3 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.