80°Csourcerecommended max constant operating temperature
Values for
LyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO values
Celanese GUR 4120 (avg. molecular weight 4.7x10^6 g/mol), typical values on compression-molded specimens; CTE and thermal conductivity from Celanese's generic UHMWPE guide (grade not named)
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Is Plastic Polypropylene stronger than Plastic UHMWPE?
Plastic Polypropylene is stronger: its yield strength is 33 MPa against 20 MPa for Plastic UHMWPE (1.65x).
Which is lighter, Plastic Polypropylene or Plastic UHMWPE?
Plastic Polypropylene is lighter: 900 kg/m³ against 930 kg/m³ for Plastic UHMWPE.
Which is stiffer, Plastic Polypropylene or Plastic UHMWPE?
Plastic Polypropylene is stiffer: Young's modulus 1.45 GPa against 0.66 GPa for Plastic UHMWPE, so the same part in Plastic Polypropylene deflects less under the same load.
Which is lighter for the same job, Plastic Polypropylene or Plastic UHMWPE?
For the same stiffness or strength: Plastic Polypropylene is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Plastic Polypropylene
Plastic UHMWPE
Stiff rod or tie (tension)
lighter
2.27x heavier
Stiff beam (bending)
lighter
1.53x heavier
Stiff panel or plate
lighter
34% heavier
Strong rod or tie
lighter
1.7x heavier
Strong beam
lighter
44% heavier
Strong panel or plate
lighter
33% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which conducts heat better, Plastic Polypropylene or Plastic UHMWPE?
Plastic UHMWPE conducts heat better: 0.4 W/m·K against 0.195 W/m·K for Plastic Polypropylene.
Which expands less with temperature?
Plastic Polypropylene expands less: 90 µm/m·K against 200 µm/m·K for Plastic UHMWPE.