Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources6 documents: Chemours, Outokumpu, Steel Construction Institute, Carpenter Technology
Plastic PTFE
Chemours Teflon PTFE 7C X granular molding resin, typical values (tensile/elongation measured on 0.13 mm skived tape)
Stainless Steel 303
1.4305 / UNS S30300, Outokumpu typical values (hot rolled, solution annealed) from 'Steel Grades, Properties and Global Standards'; max service from Carpenter CarTech 303 datasheet
1
Teflon PTFE Fluoropolymer Resin Properties HandbookChemoursarchived copyPlastic PTFE · Yield strength: typical yield strength at 23 °C (Teflon PTFE, Table 8)Plastic PTFE · Poisson's ratio: typical, 23 °C (Teflon PTFE resins, Chemours handbook)Plastic PTFE · Thermal conductivity: typical, granular resin, 4.6 mm specimenPlastic PTFE · Thermal expansion: typical, granular resin, 23-60 °C (ASTM E228)Plastic PTFE · Specific heat: typical, granular resin, 20 °C (ASTM D4591)
2
Steel Grades, Properties and Global StandardsOutokumpuarchived copyStainless Steel 303 · Yield strength: Outokumpu typical (product P = hot rolled plate, transverse)Stainless Steel 303 · Ultimate tensile strength: Outokumpu typicalStainless Steel 303 · Elongation at break: Outokumpu typical, A5Stainless Steel 303 · Young's modulus (stiffness): at RT (Table 12)Stainless Steel 303 · Density: at RTStainless Steel 303 · Thermal conductivity: at RTStainless Steel 303 · Thermal expansion: mean, 20–100 °CStainless Steel 303 · Specific heat: at RT
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 303 · Poisson's ratio: design value (structural stainless steels)
5
Teflon PTFE 6C X Product InformationChemoursarchived copyPlastic PTFE · Max service temperature: service temperature (Chemours general Teflon PTFE statement)
6
Carpenter Stainless Type 303 Data SheetCarpenter Technologyarchived copyStainless Steel 303 · Max service temperature: continuous, scaling limit
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic PTFE stronger than Stainless Steel 303?
Stainless Steel 303 is stronger: its yield strength is 275 MPa against 9 MPa for Plastic PTFE (30.6x).
Which is lighter, Plastic PTFE or Stainless Steel 303?
Plastic PTFE is lighter: 2,160 kg/m³ against 7,900 kg/m³ for Stainless Steel 303.
Which is lighter for the same job, Plastic PTFE or Stainless Steel 303?
For the same stiffness or strength: Stainless Steel 303 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Plastic PTFE
Stainless Steel 303
Strong rod or tie
8.35x heavier
lighter
Strong beam
2.67x heavier
lighter
Strong panel or plate
1.51x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PTFE or Stainless Steel 303?
Plastic PTFE stretches further before it breaks: 350% elongation at break against 35% for Stainless Steel 303.
Thermal
Which conducts heat better, Plastic PTFE or Stainless Steel 303?
Stainless Steel 303 conducts heat better: 15 W/m·K against 0.25 W/m·K for Plastic PTFE.
Which expands less with temperature?
Stainless Steel 303 expands less: 16 µm/m·K against 100 µm/m·K for Plastic PTFE.