Materials / Compare

Plywood vs. Plastic PTFE

Compare Plywood vs. Plastic PTFE strength, stiffness, weight and thermal properties.

Change either side
PlywoodNatural
Plastic PTFEBulk polymer (molded or machined)
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)9MPasourcetypical yield strength at 23 °C (Teflon PTFE, Table 8)
Ultimate tensile strength41.4MPasourcemodulus of rupture (no direct tensile value)39.3MPasourcetypical, skived tape 0.13 mm
Flexural strength41.4MPasourcestatic bending MOR (Douglas-fir); range 33.72-42.61 across speciesnot sourced
Elongation at breaknot sourced350%sourcetypical, skived tape 0.13 mm
Young's modulus (stiffness)7.45GPasourcestatic bending MOE of the panel (Douglas-fir); range 6.96-8.55 across speciesnot sourced
Densitynot sourced2,160kg/m³sourcetypical (standard specific gravity, ASTM D4894)
Strength to weightnot sourced4.17kN·m/kg
Stiffness to weightnot sourcednot sourced
Poisson's rationot sourced0.46sourcetypical, 23 °C (Teflon PTFE resins, Chemours handbook)
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourcednot sourced
Thermal
Thermal conductivity0.12W/m·KsourceAPA-recommended design value (Douglas-fir plywood), as reported by FPL/ORNL0.25W/m·Ksourcetypical, granular resin, 4.6 mm specimen
Thermal expansion3.1–4.5µm/m·Ksourcebase material: solid wood parallel to grain, ovendry, range across species100µm/m·Ksourcetypical, granular resin, 23-60 °C (ASTM E228)
100 mm part over a 50 °C swing19µm growth26.3x less500µm growth
Specific heat1,700J/kg·Ksourcebase material: solid wood (all species), 12% MC, 27 C1,400J/kg·Ksourcetypical, granular resin, 20 °C (ASTM D4591)
Heats up and cools (diffusivity)not sourced0.0827mm²/s
Thermal shock resistancenot sourcednot sourced
Melting pointnot sourced327°Csourcesecond melting peak (sintered polymer), +/-10
Max service temperaturenot sourced260°Csourceservice temperature (Chemours general Teflon PTFE statement)
Values forDouglas-fir plywood sheathing (construction plywood per PS 1), static bending properties from USDA FPL Wood Handbook FPL-GTR-282 Ch. 12 Table 12-2 (Biblis 2000)Chemours Teflon PTFE 7C X granular molding resin, typical values (tensile/elongation measured on 0.13 mm skived tape)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plywood stronger than Plastic PTFE?

Plywood is stronger: its tensile strength is 41.4 MPa against yield strength 9 MPa for Plastic PTFE (4.6x).

Which conducts heat better, Plywood or Plastic PTFE?

Plastic PTFE conducts heat better: 0.25 W/m·K against 0.12 W/m·K for Plywood.

Which expands less with temperature?

Plywood expands less: 3.8 µm/m·K against 100 µm/m·K for Plastic PTFE.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless Steel
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PTFE
Strength against density