Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: Formlabs, Outokumpu, Steel Construction Institute, Carpenter Technology
SLA Resin Tough 2000
Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.
Stainless Steel 303
1.4305 / UNS S30300, Outokumpu typical values (hot rolled, solution annealed) from 'Steel Grades, Properties and Global Standards'; max service from Carpenter CarTech 303 datasheet
Steel Grades, Properties and Global StandardsOutokumpuarchived copyStainless Steel 303 · Yield strength: Outokumpu typical (product P = hot rolled plate, transverse)Stainless Steel 303 · Ultimate tensile strength: Outokumpu typicalStainless Steel 303 · Elongation at break: Outokumpu typical, A5Stainless Steel 303 · Young's modulus (stiffness): at RT (Table 12)Stainless Steel 303 · Density: at RTStainless Steel 303 · Thermal conductivity: at RTStainless Steel 303 · Thermal expansion: mean, 20–100 °CStainless Steel 303 · Specific heat: at RT
3
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 303 · Poisson's ratio: design value (structural stainless steels)
4
Carpenter Stainless Type 303 Data SheetCarpenter Technologyarchived copyStainless Steel 303 · Max service temperature: continuous, scaling limit
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is SLA Resin Tough 2000 stronger than Stainless Steel 303?
Stainless Steel 303 is stronger: its yield strength is 275 MPa against 40.4 MPa for SLA Resin Tough 2000 (6.81x).
Which is lighter, SLA Resin Tough 2000 or Stainless Steel 303?
SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 7,900 kg/m³ for Stainless Steel 303.
Which is stiffer, SLA Resin Tough 2000 or Stainless Steel 303?
Stainless Steel 303 is stiffer: Young's modulus 200 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Stainless Steel 303 deflects less under the same load.
Which is lighter for the same job, SLA Resin Tough 2000 or Stainless Steel 303?
For the same stiffness or strength: SLA Resin Tough 2000 is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 303 is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
SLA Resin Tough 2000
Stainless Steel 303
Stiff rod or tie (tension)
15.3x heavier
lighter
Stiff beam (bending)
45% heavier
lighter
Stiff panel or plate
lighter
1.51x heavier
Strong rod or tie
lighter
6% heavier
Strong beam
lighter
2.02x heavier
Strong panel or plate
lighter
2.78x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, SLA Resin Tough 2000 or Stainless Steel 303?
SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 35% for Stainless Steel 303.
Thermal
Which expands less with temperature?
Stainless Steel 303 expands less: 16 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.