Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: Formlabs, Niagara LaSalle, U.S. Department of Defense, Ovako
SLA Resin Tough 2000
Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.
Steel AISI 1018
AISI 1018 cold drawn bar (Niagara LaSalle, cold-finished bar producer)
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 1018 · Young's modulus (stiffness): base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Density: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Poisson's ratio: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Thermal conductivity: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Specific heat: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
4
S275JR Steel GradeOvakoSteel AISI 1018 · Thermal expansion: base material: unalloyed carbon steel, Ovako family table (S275JR, 'none alloyed structural steels', C <= 0.21%); mean 20-300 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is SLA Resin Tough 2000 stronger than Steel AISI 1018?
Steel AISI 1018 is stronger: its yield strength is 372 MPa against 40.4 MPa for SLA Resin Tough 2000 (9.21x).
Which is lighter, SLA Resin Tough 2000 or Steel AISI 1018?
SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 7,861 kg/m³ for Steel AISI 1018.
Which is stiffer, SLA Resin Tough 2000 or Steel AISI 1018?
Steel AISI 1018 is stiffer: Young's modulus 200 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Steel AISI 1018 deflects less under the same load.
Which is lighter for the same job, SLA Resin Tough 2000 or Steel AISI 1018?
For the same stiffness or strength: SLA Resin Tough 2000 is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel AISI 1018 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.
Part that must be
SLA Resin Tough 2000
Steel AISI 1018
Stiff rod or tie (tension)
15.4x heavier
lighter
Stiff beam (bending)
46% heavier
lighter
Stiff panel or plate
lighter
1.5x heavier
Strong rod or tie
28% heavier
lighter
Strong beam
lighter
1.64x heavier
Strong panel or plate
lighter
2.38x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, SLA Resin Tough 2000 or Steel AISI 1018?
SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 15% for Steel AISI 1018.
Thermal
Which expands less with temperature?
Steel AISI 1018 expands less: 12 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.