Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Formlabs, Carpenter Technology, U.S. Department of Defense
SLA Resin Tough 2000
Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 4340 · Young's modulus (stiffness): MIL-HDBK-5J design value (AISI 4340, quenched and tempered)Steel AISI 4340 · Poisson's ratio: MIL-HDBK-5J design value (AISI 4340, quenched and tempered)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is SLA Resin Tough 2000 stronger than Steel AISI 4340?
Steel AISI 4340 is stronger: its yield strength is 1,035 MPa against 40.4 MPa for SLA Resin Tough 2000 (25.6x).
Which is lighter, SLA Resin Tough 2000 or Steel AISI 4340?
SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 7,840 kg/m³ for Steel AISI 4340.
Which is stiffer, SLA Resin Tough 2000 or Steel AISI 4340?
Steel AISI 4340 is stiffer: Young's modulus 200 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Steel AISI 4340 deflects less under the same load.
Which is lighter for the same job, SLA Resin Tough 2000 or Steel AISI 4340?
For the same stiffness or strength: SLA Resin Tough 2000 is lighter for a stiff panel or plate, strong panel or plate; Steel AISI 4340 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam.
Part that must be
SLA Resin Tough 2000
Steel AISI 4340
Stiff rod or tie (tension)
15.4x heavier
lighter
Stiff beam (bending)
47% heavier
lighter
Stiff panel or plate
lighter
50% heavier
Strong rod or tie
3.56x heavier
lighter
Strong beam
21% heavier
lighter
Strong panel or plate
lighter
42% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, SLA Resin Tough 2000 or Steel AISI 4340?
SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 18% for Steel AISI 4340.
Thermal
Which expands less with temperature?
Steel AISI 4340 expands less: 11.3 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.