Materials / Compare

Aluminum 6061-T6 vs. Steel A992

Compare Aluminum 6061-T6 vs. Steel A992 strength, stiffness, weight and thermal properties.

Change either side
Aluminum 6061-T6Wrought
Steel A992Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength276MPasourcetypical, 0.2% offset, .500 in dia specimen385MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISC
Ultimate tensile strength310MPasourcetypical505MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)
Elongation at break17%sourcetypical, in 4D, 0.500 in dia specimennot sourced
Young's modulus (stiffness)68.3GPasourcetypical200GPasourcedesign value (AISC 360-16)
Density2,700kg/m³sourcenominal7,850kg/m³sourcenominal (constructional data)
Strength to weight102kN·m/kg2.08x higher49kN·m/kg
Stiffness to weight25.3MN·m/kg25.5MN·m/kg
Poisson's ratio0.33sourcetypical (handbook physical constant)0.3sourcedesign value (AISC 360-16 Commentary)
Shear modulus25.7GPa76.9GPa3x stiffer in shear
Bulk modulus67GPa167GPa
Speed of sound5,030m/s5,048m/s
Thermal
Thermal conductivity167W/m·Ksourcetypical, 20 °C48W/m·Ksourcenominal at 20 °C
Thermal expansion23.6µm/m·Ksourcetypical, mean 20-100 °C12µm/m·Ksourcenominal (constructional data, no temperature range stated)
100 mm part over a 50 °C swing118µm growth60µm growth1.97x less
Specific heat896J/kg·Ksourcetypical, at 100 °C460–480J/kg·Ksourcebase material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Heats up and cools (diffusivity)69mm²/s5.31x faster13mm²/s
Thermal shock resistance19,159W/m3.55x more resistant5,390W/m
Melting point582–652°Csourcesolidus-liquidusnot sourced
Values for6061-T6/T651, Kaiser Aluminum typical properties; Poisson from MIL-HDBK-5JASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum 6061-T6 stronger than Steel A992?

Steel A992 is stronger: its yield strength is 385 MPa against 276 MPa for Aluminum 6061-T6 (39%).

Which is lighter, Aluminum 6061-T6 or Steel A992?

Aluminum 6061-T6 is lighter: 2,700 kg/m³ against 7,850 kg/m³ for Steel A992.

Which is stiffer, Aluminum 6061-T6 or Steel A992?

Steel A992 is stiffer: Young's modulus 200 GPa against 68.3 GPa for Aluminum 6061-T6, so the same part in Steel A992 deflects less under the same load.

Which is lighter for the same job, Aluminum 6061-T6 or Steel A992?

For the same stiffness or strength: Aluminum 6061-T6 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 6061-T6Steel A992
Stiff rod or tie (tension)about equalabout equal
Stiff beam (bending)lighter1.7x heavier
Stiff panel or platelighter2.03x heavier
Strong rod or tielighter2.08x heavier
Strong beamlighter2.33x heavier
Strong panel or platelighter2.46x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Aluminum 6061-T6 or Steel A992?

Aluminum 6061-T6 conducts heat better: 167 W/m·K against 48 W/m·K for Steel A992.

Which expands less with temperature?

Steel A992 expands less: 12 µm/m·K against 23.6 µm/m·K for Aluminum 6061-T6.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 6061-T6Steel A992
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 6061-T6Steel A992
Strength against density

Related comparisons