Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA panel to run stress or thermal on, free in your browser
Sources3 documents: Kaiser Aluminum, KYOCERA Fineceramics Europe, Hydro
Aluminum 1100-O
1100-O (annealed) commercially pure aluminium, Kaiser Aluminum Tube & Pipe Alloy 1100 Technical Data (Rev. 05/06), typical properties; specific heat from Hydro EN AW-1050A (99.5% Al) extruded-products datasheet (10/2018).
Ceramic Aluminum Nitride
KYOCERA AN216A dense sintered aluminium nitride, typical values; KYOCERA Fineceramics Europe data sheet 2023.04.03
1
Alloy 1100 Tube & Pipe Technical Data, Rev. 05/06Kaiser Aluminumarchived copyAluminum 1100-O · Yield strength: typical, O, 0.0625 in specimenAluminum 1100-O · Ultimate tensile strength: typical, OAluminum 1100-O · Elongation at break: typical, O, in 4DAluminum 1100-O · Young's modulus (stiffness): typicalAluminum 1100-O · Density: nominal, 20 °CAluminum 1100-O · Thermal conductivity: typical, O, 20 °CAluminum 1100-O · Thermal expansion: typical, mean 20-100 °CAluminum 1100-O · Melting point: melting range
2
AN216A Aluminium Nitride Data Sheet (2023)KYOCERA Fineceramics Europearchived copyCeramic Aluminum Nitride · Flexural strength: 3-point bending strength (JIS R 1601)Ceramic Aluminum Nitride · Young's modulus (stiffness): typical (JIS R 1602)Ceramic Aluminum Nitride · Density: typical (JIS R 1634)Ceramic Aluminum Nitride · Poisson's ratio: typical (JIS R 1602)Ceramic Aluminum Nitride · Thermal conductivity: typical (JIS R 1611)Ceramic Aluminum Nitride · Thermal expansion: mean, 40-400 °C (JIS R 1618)Ceramic Aluminum Nitride · Specific heat: typical (JIS R 1611)
3
Technical Datasheet, Extruded Products: Alloy EN AW-1050AHydroAluminum 1100-O · Specific heat: base material: commercially pure aluminium EN AW-1050A (Hydro), 20 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Which is lighter, Aluminum 1100-O or Ceramic Aluminum Nitride?
Aluminum 1100-O is lighter: 2,710 kg/m³ against 3,400 kg/m³ for Ceramic Aluminum Nitride.
Which is stiffer, Aluminum 1100-O or Ceramic Aluminum Nitride?
Ceramic Aluminum Nitride is stiffer: Young's modulus 320 GPa against 69 GPa for Aluminum 1100-O, so the same part in Ceramic Aluminum Nitride deflects less under the same load.
Which is lighter for the same job, Aluminum 1100-O or Ceramic Aluminum Nitride?
For the same stiffness or strength: Ceramic Aluminum Nitride is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.
Part that must be
Aluminum 1100-O
Ceramic Aluminum Nitride
Stiff rod or tie (tension)
3.7x heavier
lighter
Stiff beam (bending)
1.72x heavier
lighter
Stiff panel or plate
33% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Aluminum 1100-O or Ceramic Aluminum Nitride?
Aluminum 1100-O conducts heat better: 222 W/m·K against 150 W/m·K for Ceramic Aluminum Nitride.
Which expands less with temperature?
Ceramic Aluminum Nitride expands less: 4.6 µm/m·K against 23.6 µm/m·K for Aluminum 1100-O.