Materials / Compare

Aluminum 1100-O vs. Wood

Compare Aluminum 1100-O vs. Wood strength, stiffness, weight and thermal properties.

Aluminum 1100-OWrought
WoodNatural
MechanicalAluminum 1100-OWood
Yield strength35MPa1not given (tensile used)
Ultimate tensile strength90MPa1modulus of rupture99MPa2
Compressive strengthnot sourced46.6MPa2
Flexural strengthnot sourcedmodulus of rupture99MPa2
Elongation at break35%1not sourced
Young's modulus (stiffness)69GPa15.52x stifferbending MOE12.5GPa2
Density2,710kg/m³1681–702kg/m³3
Strength to weight12.9kN·m/kg143kN·m/kg11.1x higher
Stiffness to weight25.5MN·m/kg41% higher18.1MN·m/kg
Poisson's rationot sourcedmu_LR0.352
Shear modulusnot sourced4.63GPa
Bulk modulusnot sourced13.9GPa
Speed of sound5,046m/s19% faster4,252m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-OWood
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-OWood
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 1100-OWood
Thermal conductivity222W/m·K11,233x more heat through a finacross grain0.18W/m·K4
Thermal expansion23.6µm/m·K1parallel to grain3.1–4.5µm/m·K4
100 mm part over a 50 °C swing118µm growth19µm growth6.21x less
Specific heatbase material901J/kg·K5solid wood1,700J/kg·K41.89x higher
Heats up and cools (diffusivity)90.9mm²/s594x faster0.153mm²/s
Thermal shock resistancenot sourced244W/m
Melting pointmelting range640–655°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-OWood
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-OWood
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Kaiser Aluminum, USDA Forest Products Laboratory, Hydro
Aluminum 1100-O
1100-O (annealed) commercially pure aluminium, Kaiser Aluminum Tube & Pipe Alloy 1100 Technical Data (Rev. 05/06), typical properties; specific heat from Hydro EN AW-1050A (99.5% Al) extruded-products datasheet (10/2018).
Wood
Northern red oak (Quercus rubra), clear straight-grained specimens at 12% MC, parallel to grain unless stated; USDA FPL Wood Handbook FPL-GTR-282 (2021) Ch. 4 and Ch. 5
  1. 1
    Alloy 1100 Tube & Pipe Technical Data, Rev. 05/06Kaiser Aluminumarchived copyAluminum 1100-O · Yield strength: typical, O, 0.0625 in specimenAluminum 1100-O · Ultimate tensile strength: typical, OAluminum 1100-O · Elongation at break: typical, O, in 4DAluminum 1100-O · Young's modulus (stiffness): typicalAluminum 1100-O · Density: nominal, 20 °CAluminum 1100-O · Thermal conductivity: typical, O, 20 °CAluminum 1100-O · Thermal expansion: typical, mean 20-100 °CAluminum 1100-O · Melting point: melting range
  2. 2
    Wood Handbook (FPL-GTR-282), Chapter 5: Mechanical Properties of WoodUSDA Forest Products LaboratoryWood · Ultimate tensile strength: modulus of rupture (no direct tensile value)Wood · Compressive strength: compression parallel to grain (maximum crushing strength), 12% MCWood · Flexural strength: modulus of rupture (static bending), 12% MCWood · Young's modulus (stiffness): bending MOE, parallel to grainWood · Poisson's ratio: mu_LR (red oak group, ~12% MC)
  3. 3
    Technical Note 218: Weights of Various Woods Grown in the United States (1953)USDA Forest Products LaboratoryWood · Density: average weight of clear wood at 8% and 15% moisture content
  4. 4
    Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of WoodUSDA Forest Products LaboratoryWood · Thermal conductivity: across grain, 12% MC (Table 4-7, approximate)Wood · Thermal expansion: parallel to grain, ovendry wood, range across speciesWood · Specific heat: solid wood (all species), 12% MC, 27 C
  5. 5
    Technical Datasheet, Extruded Products: Alloy EN AW-1050AHydroAluminum 1100-O · Specific heat: base material: commercially pure aluminium EN AW-1050A (Hydro), 20 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 1100-O stronger than Wood?

Wood is stronger: its tensile strength is 99 MPa against yield strength 35 MPa for Aluminum 1100-O (2.83x).

Which is lighter, Aluminum 1100-O or Wood?

Wood is lighter: 692 kg/m³ against 2,710 kg/m³ for Aluminum 1100-O.

Which is stiffer, Aluminum 1100-O or Wood?

Aluminum 1100-O is stiffer: Young's modulus 69 GPa against 12.5 GPa for Wood, so the same part in Aluminum 1100-O deflects less under the same load.

Which is lighter for the same job, Aluminum 1100-O or Wood?

For the same stiffness or strength: Aluminum 1100-O is lighter for a stiff rod or tie (tension); Wood is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 1100-OWood
Stiff rod or tie (tension)lighter41% heavier
Stiff beam (bending)1.67x heavierlighter
Stiff panel or plate2.22x heavierlighter
Strong rod or tie11.1x heavierlighter
Strong beam7.84x heavierlighter
Strong panel or plate6.59x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Aluminum 1100-O or Wood?

Aluminum 1100-O conducts heat better: 222 W/m·K against 0.18 W/m·K for Wood.

Which expands less with temperature?

Wood expands less: 3.8 µm/m·K against 23.6 µm/m·K for Aluminum 1100-O.

Related comparisons