Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: Kaiser Aluminum, Cleveland-Cliffs, U.S. Department of Defense, National Institute of Standards and Technology
Aluminum 2024-T351
2024-T4/T351, Kaiser Aluminum sheet, coil & plate typical datasheet; Poisson from MIL-HDBK-5J
Iron
Cleveland-Cliffs / AK Steel ARMCO Pure Iron Product Data Bulletin (07/2022): Table 1 typical physical properties, Table 2 typical mechanical properties after SRA/recrystallization anneal.
1
Alloy 2024 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 2024-T351 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 2024-T351 · Ultimate tensile strength: typicalAluminum 2024-T351 · Elongation at break: typical, in 4DAluminum 2024-T351 · Young's modulus (stiffness): typicalAluminum 2024-T351 · Density: nominalAluminum 2024-T351 · Thermal conductivity: typical, 20 °CAluminum 2024-T351 · Thermal expansion: typical, mean 20-100 °CAluminum 2024-T351 · Specific heat: typical, at 100 °CAluminum 2024-T351 · Melting point: melting range
2
ARMCO Pure Iron Product Data Bulletin (2022)Cleveland-Cliffsarchived copyIron · Yield strength: typical (0.2% YS), hot rolled + SRA/recrystallization annealIron · Ultimate tensile strength: typical, SRA/recrystallization annealIron · Elongation at break: typical, gauge 4D0Iron · Young's modulus (stiffness): typical, after SRA/recrystallization annealIron · Density: typicalIron · Thermal conductivity: typical at 20 °CIron · Thermal expansion: mean, 20-399 °CIron · Specific heat: typicalIron · Melting point: typical
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 2024-T351 · Poisson's ratio: typical (handbook physical constant), all tempers
4
Elastic Properties of Metals and Alloys, I. Iron, Nickel, and Iron-Nickel Alloys, J. Phys. Chem. Ref. Data 2 (1973)National Institute of Standards and Technologyarchived copyIron · Poisson's ratio: NIST critically evaluated best value (polycrystalline iron)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 2024-T351 stronger than Iron?
Aluminum 2024-T351 is stronger: its yield strength is 324 MPa against 186 MPa for Iron (1.74x).
Which is lighter, Aluminum 2024-T351 or Iron?
Aluminum 2024-T351 is lighter: 2,770 kg/m³ against 7,860 kg/m³ for Iron.
Which is stiffer, Aluminum 2024-T351 or Iron?
Iron is stiffer: Young's modulus 207 GPa against 73.1 GPa for Aluminum 2024-T351, so the same part in Iron deflects less under the same load.
Which is lighter for the same job, Aluminum 2024-T351 or Iron?
For the same stiffness or strength: Aluminum 2024-T351 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 2024-T351
Iron
Stiff rod or tie (tension)
about equal
about equal
Stiff beam (bending)
lighter
1.69x heavier
Stiff panel or plate
lighter
2.01x heavier
Strong rod or tie
lighter
4.94x heavier
Strong beam
lighter
4.11x heavier
Strong panel or plate
lighter
3.75x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 2024-T351 or Iron?
Iron stretches further before it breaks: 38% elongation at break against 19% for Aluminum 2024-T351.
Thermal
Which conducts heat better, Aluminum 2024-T351 or Iron?
Aluminum 2024-T351 conducts heat better: 120 W/m·K against 73.2 W/m·K for Iron.
Which expands less with temperature?
Iron expands less: 13.7 µm/m·K against 22.9 µm/m·K for Aluminum 2024-T351.