Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Kaiser Aluminum, Covestro, U.S. Department of Defense, Bayer MaterialScience
Aluminum 5052-H32
5052-H32, Kaiser Aluminum tube & pipe typical datasheet (mechanical, CTE, melting); MIL-HDBK-5J (Poisson, density, specific heat)
Plastic Polycarbonate
Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values
1
Alloy 5052 Tube & Pipe Technical DataKaiser Aluminumarchived copyAluminum 5052-H32 · Yield strength: typical, 0.2% offsetAluminum 5052-H32 · Ultimate tensile strength: typicalAluminum 5052-H32 · Elongation at break: typicalAluminum 5052-H32 · Young's modulus (stiffness): typicalAluminum 5052-H32 · Thermal conductivity: base material: 5052 in O temper (same alloy, annealed); Kaiser typicalAluminum 5052-H32 · Thermal expansion: typical, mean 20-100 °CAluminum 5052-H32 · Melting point: melting range
2
Makrolon 2405 Technical Data SheetCovestroPlastic Polycarbonate · Yield strength: typical, tensile yieldPlastic Polycarbonate · Ultimate tensile strength: typical, stress at breakPlastic Polycarbonate · Flexural strength: typical, flexural strengthPlastic Polycarbonate · Elongation at break: typical, strain at breakPlastic Polycarbonate · Young's modulus (stiffness): typicalPlastic Polycarbonate · Density: typicalPlastic Polycarbonate · Thermal conductivity: typical, through-plane, 23 CPlastic Polycarbonate · Thermal expansion: typical, 23-55 C, parallel and normalPlastic Polycarbonate · Glass transition: typical, DSC 10 C/minPlastic Polycarbonate · Max service temperature: UL 746B RTI, tensile strength, 1.5 mm
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 5052-H32 · Density: nominalAluminum 5052-H32 · Poisson's ratio: typical (handbook physical constant)Aluminum 5052-H32 · Specific heat: at 100 °C (212 °F); table covers O, H32, H34, H36, H38
4
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
5
Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 5052-H32 stronger than Plastic Polycarbonate?
Aluminum 5052-H32 is stronger: its yield strength is 195 MPa against 65 MPa for Plastic Polycarbonate (3x).
Which is lighter, Aluminum 5052-H32 or Plastic Polycarbonate?
Plastic Polycarbonate is lighter: 1,200 kg/m³ against 2,685 kg/m³ for Aluminum 5052-H32.
Which is stiffer, Aluminum 5052-H32 or Plastic Polycarbonate?
Aluminum 5052-H32 is stiffer: Young's modulus 70 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Aluminum 5052-H32 deflects less under the same load.
Which is lighter for the same job, Aluminum 5052-H32 or Plastic Polycarbonate?
For the same stiffness or strength: Aluminum 5052-H32 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie; Plastic Polycarbonate is lighter for a strong beam, strong panel or plate.
Part that must be
Aluminum 5052-H32
Plastic Polycarbonate
Stiff rod or tie (tension)
lighter
13x heavier
Stiff beam (bending)
lighter
2.41x heavier
Stiff panel or plate
lighter
38% heavier
Strong rod or tie
lighter
34% heavier
Strong beam
8% heavier
lighter
Strong panel or plate
29% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 5052-H32 or Plastic Polycarbonate?
Plastic Polycarbonate stretches further before it breaks: 125% elongation at break against 12% for Aluminum 5052-H32.
Thermal
Which conducts heat better, Aluminum 5052-H32 or Plastic Polycarbonate?
Aluminum 5052-H32 conducts heat better: 138 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.
Which expands less with temperature?
Aluminum 5052-H32 expands less: 23.8 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.