Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Kaiser Aluminum, Formlabs, U.S. Department of Defense
Aluminum 5052-H32
5052-H32, Kaiser Aluminum tube & pipe typical datasheet (mechanical, CTE, melting); MIL-HDBK-5J (Poisson, density, specific heat)
SLA Resin Tough 2000
Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.
1
Alloy 5052 Tube & Pipe Technical DataKaiser Aluminumarchived copyAluminum 5052-H32 · Yield strength: typical, 0.2% offsetAluminum 5052-H32 · Ultimate tensile strength: typicalAluminum 5052-H32 · Elongation at break: typicalAluminum 5052-H32 · Young's modulus (stiffness): typicalAluminum 5052-H32 · Thermal conductivity: base material: 5052 in O temper (same alloy, annealed); Kaiser typicalAluminum 5052-H32 · Thermal expansion: typical, mean 20-100 °CAluminum 5052-H32 · Melting point: melting range
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 5052-H32 · Density: nominalAluminum 5052-H32 · Poisson's ratio: typical (handbook physical constant)Aluminum 5052-H32 · Specific heat: at 100 °C (212 °F); table covers O, H32, H34, H36, H38
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 5052-H32 stronger than SLA Resin Tough 2000?
Aluminum 5052-H32 is stronger: its yield strength is 195 MPa against 40.4 MPa for SLA Resin Tough 2000 (4.83x).
Which is lighter, Aluminum 5052-H32 or SLA Resin Tough 2000?
SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 2,685 kg/m³ for Aluminum 5052-H32.
Which is stiffer, Aluminum 5052-H32 or SLA Resin Tough 2000?
Aluminum 5052-H32 is stiffer: Young's modulus 70 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Aluminum 5052-H32 deflects less under the same load.
Which is lighter for the same job, Aluminum 5052-H32 or SLA Resin Tough 2000?
For the same stiffness or strength: Aluminum 5052-H32 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam; SLA Resin Tough 2000 is lighter for a strong panel or plate.
Part that must be
Aluminum 5052-H32
SLA Resin Tough 2000
Stiff rod or tie (tension)
lighter
15.8x heavier
Stiff beam (bending)
lighter
2.53x heavier
Stiff panel or plate
lighter
38% heavier
Strong rod or tie
lighter
1.96x heavier
Strong beam
lighter
16% heavier
Strong panel or plate
12% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 5052-H32 or SLA Resin Tough 2000?
SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 12% for Aluminum 5052-H32.
Thermal
Which expands less with temperature?
Aluminum 5052-H32 expands less: 23.8 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.