Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Alloy 7075 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 7075-T6 · Density: nominalAluminum 7075-T6 · Thermal conductivity: typical, 20 °C, T651Aluminum 7075-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 7075-T6 · Specific heat: typical, at 100 °CAluminum 7075-T6 · Melting point: melting range
4
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7075-T6 · Poisson's ratio: typical (handbook physical constant)
5
Wieland-K32 (Cu-ETP, C11000) Data SheetWielandarchived copyCopper C110 · Poisson's ratio: reference value at room temperature (Wieland-K32 = Cu-ETP = C11000, rolled products)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 7075-T6 stronger than Copper C110?
Aluminum 7075-T6 is stronger: its yield strength is 503 MPa against 69 MPa for Copper C110 (7.29x).
Which is lighter, Aluminum 7075-T6 or Copper C110?
Aluminum 7075-T6 is lighter: 2,800 kg/m³ against 8,913 kg/m³ for Copper C110.
Which is stiffer, Aluminum 7075-T6 or Copper C110?
Copper C110 is stiffer: Young's modulus 117 GPa against 71 GPa for Aluminum 7075-T6, so the same part in Copper C110 deflects less under the same load.
Which is lighter for the same job, Aluminum 7075-T6 or Copper C110?
For the same stiffness or strength: Aluminum 7075-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 7075-T6
Copper C110
Stiff rod or tie (tension)
lighter
1.93x heavier
Stiff beam (bending)
lighter
2.48x heavier
Stiff panel or plate
lighter
2.69x heavier
Strong rod or tie
lighter
23.2x heavier
Strong beam
lighter
12x heavier
Strong panel or plate
lighter
8.59x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 7075-T6 or Copper C110?
Copper C110 stretches further before it breaks: 55% elongation at break against 11% for Aluminum 7075-T6.
Thermal
Which conducts heat better, Aluminum 7075-T6 or Copper C110?
Copper C110 conducts heat better: 391 W/m·K against 130 W/m·K for Aluminum 7075-T6.
Which expands less with temperature?
Copper C110 expands less: 16.9 µm/m·K against 23.4 µm/m·K for Aluminum 7075-T6.