Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Alloy 7075 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 7075-T6 · Density: nominalAluminum 7075-T6 · Thermal conductivity: typical, 20 °C, T651Aluminum 7075-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 7075-T6 · Specific heat: typical, at 100 °CAluminum 7075-T6 · Melting point: melting range
4
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7075-T6 · Poisson's ratio: typical (handbook physical constant)
5
Engineering Properties of Ingeo BiopolymerNatureWorksarchived copyPlastic PLA · Thermal conductivity: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °CPlastic PLA · Specific heat: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Plastic PLA is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 7075-T6 stronger than Plastic PLA?
Aluminum 7075-T6 is stronger: its yield strength is 503 MPa against 52.5 MPa for Plastic PLA (9.58x).
Which is lighter, Aluminum 7075-T6 or Plastic PLA?
Plastic PLA is lighter: 1,240 kg/m³ against 2,800 kg/m³ for Aluminum 7075-T6.
Which is stiffer, Aluminum 7075-T6 or Plastic PLA?
Aluminum 7075-T6 is stiffer: Young's modulus 71 GPa against 3.25 GPa for Plastic PLA, so the same part in Aluminum 7075-T6 deflects less under the same load.
Which is lighter for the same job, Aluminum 7075-T6 or Plastic PLA?
For the same stiffness or strength: Aluminum 7075-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 7075-T6
Plastic PLA
Stiff rod or tie (tension)
lighter
9.67x heavier
Stiff beam (bending)
lighter
2.07x heavier
Stiff panel or plate
lighter
24% heavier
Strong rod or tie
lighter
4.24x heavier
Strong beam
lighter
2x heavier
Strong panel or plate
lighter
37% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 7075-T6 or Plastic PLA?
Aluminum 7075-T6 stretches further before it breaks: 11% elongation at break against 7.8% for Plastic PLA.
Thermal
Which conducts heat better, Aluminum 7075-T6 or Plastic PLA?
Aluminum 7075-T6 conducts heat better: 130 W/m·K against 0.13 W/m·K for Plastic PLA.