Materials / Compare

Aluminum A380 vs. Ceramic Aluminum Nitride

Compare Aluminum A380 vs. Ceramic Aluminum Nitride strength, stiffness, weight and thermal properties.

Aluminum A380Cast
Ceramic Aluminum NitrideSintered ceramic (pressed and fired)
MechanicalAluminum A380Ceramic Aluminum Nitride
Yield strength160MPa1none (brittle)
Ultimate tensile strength320MPa1not sourced
Flexural strengthnot sourced310MPa2
Elongation at break3.5%1none (brittle)
Young's modulus (stiffness)71GPa1320GPa24.51x stiffer
Density2,713kg/m³125% lighter3,400kg/m³2
Strength to weight59kN·m/kgnot sourced
Stiffness to weight26.2MN·m/kg94.1MN·m/kg3.6x higher
Poisson's ratio0.3330.242
Shear modulus26.7GPa129GPa4.83x stiffer in shear
Bulk modulus69.6GPa205GPa2.95x higher
Speed of sound5,116m/s9,701m/s1.9x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum A380Ceramic Aluminum Nitride
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum A380
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum A380Ceramic Aluminum Nitride
Thermal conductivity96.2W/m·K1150W/m·K21.56x more heat through a fin
Thermal expansion21.8µm/m·K1mean4.6µm/m·K24.73x less
100 mm part over a 50 °C swing109µm growth23µm growth4.73x less
Specific heat963J/kg·K136% higher710J/kg·K2
Heats up and cools (diffusivity)36.8mm²/s62.1mm²/s1.69x faster
Thermal shock resistance6,669W/mnot sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum A380Ceramic Aluminum Nitride
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum A380Ceramic Aluminum Nitride
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Rheocast Company, KYOCERA Fineceramics Europe, North American Die Casting Association
Aluminum A380
A380 aluminium high-pressure die-casting alloy, typical properties; Rheocast Company (aluminium die caster, Germantown WI) A380 alloy data page.
Ceramic Aluminum Nitride
KYOCERA AN216A dense sintered aluminium nitride, typical values; KYOCERA Fineceramics Europe data sheet 2023.04.03
  1. 1
    Alloy Aluminum: A380Rheocast CompanyAluminum A380 · Yield strength: typical, 25 °CAluminum A380 · Ultimate tensile strength: typical, 25 °CAluminum A380 · Elongation at break: typicalAluminum A380 · Young's modulus (stiffness): typical, 25 °CAluminum A380 · Density: typical at 68 °FAluminum A380 · Thermal conductivity: typical at 68 °FAluminum A380 · Thermal expansion: typical, 68-572 °F (20-300 °C)Aluminum A380 · Specific heat: typical at 68 °F
  2. 2
    AN216A Aluminium Nitride Data Sheet (2023)KYOCERA Fineceramics Europearchived copyCeramic Aluminum Nitride · Flexural strength: 3-point bending strength (JIS R 1601)Ceramic Aluminum Nitride · Young's modulus (stiffness): typical (JIS R 1602)Ceramic Aluminum Nitride · Density: typical (JIS R 1634)Ceramic Aluminum Nitride · Poisson's ratio: typical (JIS R 1602)Ceramic Aluminum Nitride · Thermal conductivity: typical (JIS R 1611)Ceramic Aluminum Nitride · Thermal expansion: mean, 40-400 °C (JIS R 1618)Ceramic Aluminum Nitride · Specific heat: typical (JIS R 1611)
  3. 3
    Product Design for Die Casting, Table 4.1: Die Casting Alloys Material Properties ComparisonNorth American Die Casting Associationarchived copyAluminum A380 · Poisson's ratio: typical, as-cast, separately die cast specimens

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Which is lighter, Aluminum A380 or Ceramic Aluminum Nitride?

Aluminum A380 is lighter: 2,713 kg/m³ against 3,400 kg/m³ for Ceramic Aluminum Nitride.

Which is stiffer, Aluminum A380 or Ceramic Aluminum Nitride?

Ceramic Aluminum Nitride is stiffer: Young's modulus 320 GPa against 71 GPa for Aluminum A380, so the same part in Ceramic Aluminum Nitride deflects less under the same load.

Which is lighter for the same job, Aluminum A380 or Ceramic Aluminum Nitride?

For the same stiffness or strength: Ceramic Aluminum Nitride is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beAluminum A380Ceramic Aluminum Nitride
Stiff rod or tie (tension)3.6x heavierlighter
Stiff beam (bending)1.69x heavierlighter
Stiff panel or plate32% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Aluminum A380 or Ceramic Aluminum Nitride?

Ceramic Aluminum Nitride conducts heat better: 150 W/m·K against 96.2 W/m·K for Aluminum A380.

Which expands less with temperature?

Ceramic Aluminum Nitride expands less: 4.6 µm/m·K against 21.8 µm/m·K for Aluminum A380.

Related comparisons