Materials / Compare

Aluminum ADC12 vs. SLA Resin Elastic 50A

Compare Aluminum ADC12 vs. SLA Resin Elastic 50A strength, stiffness, weight and thermal properties.

Aluminum ADC12Cast
SLA Resin Elastic 50A3D printed (SLA resin)
MechanicalAluminum ADC12SLA Resin Elastic 50A
Yield strengthone test result149MPa1not given (tensile used)
Ultimate tensile strengthone test result345MPa1101x stronger3.4MPa2
Elongation at breakone test result2.3%1160%269.6x more ductile
Young's modulus (stiffness)standard value79.8GPa3not sourced
Densitymeasured2,680kg/m³41,010kg/m³22.65x lighter
Strength to weight55.6kN·m/kg16.5x higher3.37kN·m/kg
Stiffness to weight29.8MN·m/kgnot sourced
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound5,457m/snot sourced
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OMagnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum ADC12
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OMagnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum ADC12SLA Resin Elastic 50A
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum ADC12SLA Resin Elastic 50A
Thermal conductivity125W/m·K4not sourced
Thermal expansionmeasured21µm/m·K4not sourced
100 mm part over a 50 °C swing105µm growthnot sourced
Specific heatmeasured911J/kg·K4not sourced
Heats up and cools (diffusivity)51.2mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Melting pointsolidus-liquidus515–582°C4not sourced
Glass transitionnot sourcedDMA-34.5°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OMagnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum ADC12
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OMagnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum ADC12
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Daiki Aluminium Industry, Formlabs, S.S. Aluminum
Aluminum ADC12
JIS ADC12 (Al-Si-Cu, about A383 / EN AC-46100) high-pressure die-casting alloy, as cast; physical properties from Daiki Aluminium Industry (ADC12 ingot producer) measured values; modulus from S.S.Aluminum (ADC12 ingot producer) standard values.
SLA Resin Elastic 50A
Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.
  1. 1
    NA Alloys Product DataDaiki Aluminium IndustryAluminum ADC12 · Yield strength: one test result, 0.2% proof stress, as cast, ASTM tensile bar (Daiki)Aluminum ADC12 · Ultimate tensile strength: one test result, as cast, ASTM tensile bar (Daiki)Aluminum ADC12 · Elongation at break: one test result, as cast, ASTM tensile bar (Daiki)
  2. 2
    Elastic 50A Resin V2 Technical Data Sheet (2024)Formlabsarchived copySLA Resin Elastic 50A · Ultimate tensile strength: typicalSLA Resin Elastic 50A · Elongation at break: typicalSLA Resin Elastic 50A · Density: typicalSLA Resin Elastic 50A · Glass transition: DMA
  3. 3
    Die-Casting Alloys (ダイカスト用合金)S.S. AluminumAluminum ADC12 · Young's modulus (stiffness): standard value (S.S.Aluminum)
  4. 4
    DIK365 Product DataDaiki Aluminium IndustryAluminum ADC12 · Density: measured (Daiki)Aluminum ADC12 · Thermal conductivity: measured on specimens cut from a 50 x 100 x 5 mm flat die casting (Daiki)Aluminum ADC12 · Thermal expansion: measured, temperature range not stated (Daiki)Aluminum ADC12 · Specific heat: measured (Daiki)Aluminum ADC12 · Melting point: solidus-liquidus (Daiki)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Aluminum ADC12 stronger than SLA Resin Elastic 50A?

Aluminum ADC12 is stronger: its yield strength is 149 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (43.8x).

Which is lighter, Aluminum ADC12 or SLA Resin Elastic 50A?

SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 2,680 kg/m³ for Aluminum ADC12.

Which is lighter for the same job, Aluminum ADC12 or SLA Resin Elastic 50A?

For the same stiffness or strength: Aluminum ADC12 is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum ADC12SLA Resin Elastic 50A
Strong rod or tielighter16.5x heavier
Strong beamlighter4.68x heavier
Strong panel or platelighter2.49x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum ADC12 or SLA Resin Elastic 50A?

SLA Resin Elastic 50A stretches further before it breaks: 160% elongation at break against 2.3% for Aluminum ADC12.

Related comparisons