Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
JIS ADC12 (Al-Si-Cu, about A383 / EN AC-46100) high-pressure die-casting alloy, as cast; physical properties from Daiki Aluminium Industry (ADC12 ingot producer) measured values; modulus from S.S.Aluminum (ADC12 ingot producer) standard values.
SLA Resin Standard
Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.
1
NA Alloys Product DataDaiki Aluminium IndustryAluminum ADC12 · Yield strength: one test result, 0.2% proof stress, as cast, ASTM tensile bar (Daiki)Aluminum ADC12 · Ultimate tensile strength: one test result, as cast, ASTM tensile bar (Daiki)Aluminum ADC12 · Elongation at break: one test result, as cast, ASTM tensile bar (Daiki)
2
Clear Resin V5 Technical Data Sheet (2024)Formlabsarchived copySLA Resin Standard · Ultimate tensile strength: typicalSLA Resin Standard · Flexural strength: typicalSLA Resin Standard · Elongation at break: typicalSLA Resin Standard · Young's modulus (stiffness): typicalSLA Resin Standard · Max service temperature: HDT 1.8 MPa
3
Die-Casting Alloys (ダイカスト用合金)S.S. AluminumAluminum ADC12 · Young's modulus (stiffness): standard value (S.S.Aluminum)
4
DIK365 Product DataDaiki Aluminium IndustryAluminum ADC12 · Density: measured (Daiki)Aluminum ADC12 · Thermal conductivity: measured on specimens cut from a 50 x 100 x 5 mm flat die casting (Daiki)Aluminum ADC12 · Thermal expansion: measured, temperature range not stated (Daiki)Aluminum ADC12 · Specific heat: measured (Daiki)Aluminum ADC12 · Melting point: solidus-liquidus (Daiki)
5
Clear Resin V5 Technical Data Sheet (web edition)FormlabsSLA Resin Standard · Density: typical, post-cured (same for 5 min ambient and 15 min at 60 °C), ASTM D792
6
Thermal Properties of Selected Formlabs SLA ResinsFormlabsSLA Resin Standard · Thermal conductivity: typical, post-cured, ASTM E1530SLA Resin Standard · Thermal expansion: mean -30 to 140 °C, post-cured (5 min ambient cure), TMA ASTM E831SLA Resin Standard · Specific heat: typical, 25 °C, post-cured (5 min ambient cure), DSC ASTM E1269
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum ADC12 stronger than SLA Resin Standard?
Aluminum ADC12 is stronger: its yield strength is 149 MPa against tensile strength 60 MPa for SLA Resin Standard (2.48x).
Which is lighter, Aluminum ADC12 or SLA Resin Standard?
SLA Resin Standard is lighter: 1,210 kg/m³ against 2,680 kg/m³ for Aluminum ADC12.
Which is stiffer, Aluminum ADC12 or SLA Resin Standard?
Aluminum ADC12 is stiffer: Young's modulus 79.8 GPa against 2.75 GPa for SLA Resin Standard, so the same part in Aluminum ADC12 deflects less under the same load.
Which is lighter for the same job, Aluminum ADC12 or SLA Resin Standard?
For the same stiffness or strength: Aluminum ADC12 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie; SLA Resin Standard is lighter for a strong beam, strong panel or plate.
Part that must be
Aluminum ADC12
SLA Resin Standard
Stiff rod or tie (tension)
lighter
13.1x heavier
Stiff beam (bending)
lighter
2.43x heavier
Stiff panel or plate
lighter
39% heavier
Strong rod or tie
lighter
12% heavier
Strong beam
21% heavier
lighter
Strong panel or plate
41% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum ADC12 or SLA Resin Standard?
SLA Resin Standard stretches further before it breaks: 8% elongation at break against 2.3% for Aluminum ADC12.
Thermal
Which conducts heat better, Aluminum ADC12 or SLA Resin Standard?
Aluminum ADC12 conducts heat better: 125 W/m·K against 0.54 W/m·K for SLA Resin Standard.
Which expands less with temperature?
Aluminum ADC12 expands less: 21 µm/m·K against 114 µm/m·K for SLA Resin Standard.