Materials / Compare
Aluminum vs. DMLS Ti-6Al-4V ELI Titanium
Compare Aluminum vs. DMLS Ti-6Al-4V ELI Titanium strength, stiffness, weight and thermal properties.
| Mechanical | Aluminum | DMLS Ti-6Al-4V ELI Titanium |
|---|---|---|
| Yield strength | 276MPa1 | 1,100MPa23.99x stronger |
| Ultimate tensile strength | 310MPa1 | 1,270MPa24.1x stronger |
| Elongation at break | 17%11.95x more ductile | 8.7%2 |
| Young's modulus (stiffness) | 68.3GPa1 | same maker and process110GPa31.61x stiffer |
| Density | 2,700kg/m³11.63x lighter | 4,400kg/m³2 |
| Strength to weight | 102kN·m/kg | 250kN·m/kg2.45x higher |
| Stiffness to weight | 25.3MN·m/kg1% higher | 25MN·m/kg |
| Poisson's ratio | 0.334 | wrought TIMETAL 6-40.3425 |
| Shear modulus | 25.7GPa | 41GPa1.6x stiffer in shear |
| Bulk modulus | 67GPa | 116GPa1.73x higher |
| Speed of sound | 5,030m/s | 5,000m/s |
| Thermal | Aluminum | DMLS Ti-6Al-4V ELI Titanium |
|---|---|---|
| Thermal conductivity | 167W/m·K125.3x more heat through a fin | base material6.6W/m·K6 |
| Thermal expansion | 23.6µm/m·K1 | mean 25-100 °C9µm/m·K72.62x less |
| 100 mm part over a 50 °C swing | 118µm growth | 45µm growth2.62x less |
| Specific heat | 896J/kg·K11.54x higher | base material580J/kg·K6 |
| Heats up and cools (diffusivity) | 69mm²/s26.7x faster | 2.59mm²/s |
| Thermal shock resistance | 19,159W/m3.97x more resistant | 4,825W/m |
| Melting point | solidus-liquidus582–652°C1 | melting range1,630–1,650°C5 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources7 documents: Kaiser Aluminum, EOS GmbH, U.S. Department of Defense, TIMET
- Aluminum
- 6061-T6/T651, Kaiser Aluminum typical properties (sheet, coil & plate datasheet); Poisson from MIL-HDBK-5J
- DMLS Ti-6Al-4V ELI Titanium
- EOS Titanium Ti64ELI (powder 9011-0040; ASTM F136/F3001, i.e. Grade 23) on EOS M400 SF, parameter set Ti64ELI_030_FlexM400_100, 30 µm, as built; ISO 6892-1 A14
- 1Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum · Ultimate tensile strength: typicalAluminum · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum · Young's modulus (stiffness): typicalAluminum · Density: nominalAluminum · Thermal conductivity: typical, 20 °CAluminum · Thermal expansion: typical, mean 20-100 °CAluminum · Specific heat: typical, at 100 °CAluminum · Melting point: solidus-liquidus
- 2EOS Titanium Ti64ELI Material Data Sheet, M 290 and M 400EOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Yield strength: typical, as built, average of horizontal + vertical (M400)DMLS Ti-6Al-4V ELI Titanium · Ultimate tensile strength: typical, as built, average of horizontal + vertical (M400)DMLS Ti-6Al-4V ELI Titanium · Elongation at break: typical at break, as built (M400)DMLS Ti-6Al-4V ELI Titanium · Density: typical part density (ISO 3369), M400
- 3EOS Titanium Ti64 Material Data Sheet, M 290 (2022)EOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Young's modulus (stiffness): same maker and process, sibling grade: EOS Titanium Ti64 (Grade 5) on EOS M 290, as built, XY and Z, typical
- 4MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum · Poisson's ratio: typical (handbook physical constant)
- 5TIMETAL 6-4 PropertiesTIMETarchived copyDMLS Ti-6Al-4V ELI Titanium · Poisson's ratio: wrought TIMETAL 6-4 (TIMET measurement, mean of 10); composition-level, not DMLS-measuredDMLS Ti-6Al-4V ELI Titanium · Melting point: melting range, wrought TIMETAL 6-4 (composition-level)
- 6TIMETAL 6-4 Data SheetTIMETarchived copyDMLS Ti-6Al-4V ELI Titanium · Thermal conductivity: base material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °CDMLS Ti-6Al-4V ELI Titanium · Specific heat: base material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
- 7EOS Titanium Ti64 Grade 23 Material Data SheetEOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Thermal expansion: mean 25-100 °C, ASTM E228; EOS Ti64 Grade 23 (=ELI) on EOS M 290 40 µm; condition not stated (sheet's mechanical data are heat treated)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS Ti-6Al-4V ELI Titanium is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum stronger than DMLS Ti-6Al-4V ELI Titanium?
DMLS Ti-6Al-4V ELI Titanium is stronger: its yield strength is 1,100 MPa against 276 MPa for Aluminum (3.99x).
Which is lighter, Aluminum or DMLS Ti-6Al-4V ELI Titanium?
Aluminum is lighter: 2,700 kg/m³ against 4,400 kg/m³ for DMLS Ti-6Al-4V ELI Titanium.
Which is stiffer, Aluminum or DMLS Ti-6Al-4V ELI Titanium?
DMLS Ti-6Al-4V ELI Titanium is stiffer: Young's modulus 110 GPa against 68.3 GPa for Aluminum, so the same part in DMLS Ti-6Al-4V ELI Titanium deflects less under the same load.
Which is lighter for the same job, Aluminum or DMLS Ti-6Al-4V ELI Titanium?
For the same stiffness or strength: Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; DMLS Ti-6Al-4V ELI Titanium is lighter for a strong rod or tie, strong beam, strong panel or plate.
| Part that must be | Aluminum | DMLS Ti-6Al-4V ELI Titanium |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 1% heavier |
| Stiff beam (bending) | lighter | 28% heavier |
| Stiff panel or plate | lighter | 39% heavier |
| Strong rod or tie | 2.45x heavier | lighter |
| Strong beam | 1.54x heavier | lighter |
| Strong panel or plate | 23% heavier | lighter |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum or DMLS Ti-6Al-4V ELI Titanium?
Aluminum stretches further before it breaks: 17% elongation at break against 8.7% for DMLS Ti-6Al-4V ELI Titanium.
Thermal
Which conducts heat better, Aluminum or DMLS Ti-6Al-4V ELI Titanium?
Aluminum conducts heat better: 167 W/m·K against 6.6 W/m·K for DMLS Ti-6Al-4V ELI Titanium.
Which expands less with temperature?
DMLS Ti-6Al-4V ELI Titanium expands less: 9 µm/m·K against 23.6 µm/m·K for Aluminum.
Related comparisons
- Aluminum vs. Aluminum 6061-T6
- Aluminum vs. DMLS AlSi10Mg Aluminum
- Aluminum vs. Aluminum 2024-T351
- Aluminum vs. Aluminum 6063-T6
- DMLS Ti-6Al-4V ELI Titanium vs. Titanium
- DMLS Ti-6Al-4V ELI Titanium vs. Titanium Ti-6Al-4V
- DMLS Ti-6Al-4V ELI Titanium vs. Stainless Steel 17-4PH
- DMLS Ti-6Al-4V ELI Titanium vs. Steel AISI 4340