Materials / DMLS

DMLS Ti-6Al-4V ELI Titanium

DMLS Ti-6Al-4V ELI Titanium strength, stiffness, density and thermal properties, with their source.

A bracket in DMLS Ti-6Al-4V ELI Titanium, as-sintered finish.

Process3D printed metal (DMLS)
Mechanical
Yield strength1,100MPasourcetypical, as built, average of horizontal + vertical (M400)
Ultimate tensile strength1,270MPasourcetypical, as built, average of horizontal + vertical (M400)
Elongation at break8.7%sourcetypical at break, as built (M400)
Young's modulus (stiffness)110GPasourcesame maker and process, sibling grade: EOS Titanium Ti64 (Grade 5) on EOS M 290, as built, XY and Z, typical
Density4,400kg/m³sourcetypical part density (ISO 3369), M400
Strength to weight250kN·m/kg
Stiffness to weight25MN·m/kg
Poisson's ratio0.342sourcewrought TIMETAL 6-4 (TIMET measurement, mean of 10); composition-level, not DMLS-measured
Shear modulus41GPa
Bulk modulus116GPa
Speed of sound5,000m/s
Thermal
Thermal conductivity6.6W/m·Ksourcebase material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
Thermal expansion9µm/m·Ksourcemean 25-100 °C, ASTM E228; EOS Ti64 Grade 23 (=ELI) on EOS M 290 40 µm; condition not stated (sheet's mechanical data are heat treated)
100 mm part over a 50 °C swing45µm growth
Specific heat580J/kg·Ksourcebase material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
Heats up and cools (diffusivity)2.59mm²/s
Thermal shock resistance4,825W/m
Melting point1,630–1,650°Csourcemelting range, wrought TIMETAL 6-4 (composition-level)
Values forEOS Titanium Ti64ELI (powder 9011-0040; ASTM F136/F3001, i.e. Grade 23) on EOS M400 SF, parameter set Ti64ELI_030_FlexM400_100, 30 µm, as built; ISO 6892-1 A14

DMLS Ti-6Al-4V ELI Titanium is 3D printed: its properties depend on build direction and print settings; these are typical values.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelDMLS Ti-6Al-4V ELI Titanium
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickDMLS Ti-6Al-4V ELI Titanium
Strength against density

Compare DMLS Ti-6Al-4V ELI Titanium with