Materials / Compare

DMLS 316L Stainless Steel vs. DMLS Ti-6Al-4V ELI Titanium

Compare DMLS 316L Stainless Steel vs. DMLS Ti-6Al-4V ELI Titanium strength, stiffness, weight and thermal properties.

Change either side
DMLS 316L Stainless Steel3D printed metal (DMLS)
DMLS Ti-6Al-4V ELI Titanium3D printed metal (DMLS)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength530MPasourcetypical, as manufactured, horizontal1,100MPasourcetypical, as built, average of horizontal + vertical (M400)
Ultimate tensile strength640MPasourcetypical, as manufactured, horizontal1,270MPasourcetypical, as built, average of horizontal + vertical (M400)
Elongation at break40%sourcetypical at break, as manufactured, horizontal8.7%sourcetypical at break, as built (M400)
Young's modulus (stiffness)185GPasourcetypical, as built, horizontal (XY); EOSINT M280-400W / M290-400W, 316L_Surface 1.0, 20 µm (2014 sheet)110GPasourcesame maker and process, sibling grade: EOS Titanium Ti64 (Grade 5) on EOS M 290, as built, XY and Z, typical
Density7,900kg/m³sourcepart density (ISO 3369, not labelled min or typical), EOS M 290, 40 µm FlexLine4,400kg/m³sourcetypical part density (ISO 3369), M400
Strength to weight67.1kN·m/kg250kN·m/kg3.73x higher
Stiffness to weight23.4MN·m/kg25MN·m/kg7% higher
Poisson's ratio0.3sourcebase material: austenitic stainless steels incl. 1.4404 (316L), design value0.342sourcewrought TIMETAL 6-4 (TIMET measurement, mean of 10); composition-level, not DMLS-measured
Shear modulus71.2GPa1.74x stiffer in shear41GPa
Bulk modulus154GPa116GPa
Speed of sound4,839m/s5,000m/s
Thermal
Thermal conductivity16.2W/m·Ksourcebase material: wrought 316/316L (Cleveland-Cliffs), at 100 °C6.6W/m·Ksourcebase material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
Thermal expansion15.7µm/m·Ksourcemean 25-100 °C, ASTM E2289µm/m·Ksourcemean 25-100 °C, ASTM E228; EOS Ti64 Grade 23 (=ELI) on EOS M 290 40 µm; condition not stated (sheet's mechanical data are heat treated)
100 mm part over a 50 °C swing78.6µm growth45µm growth1.75x less
Specific heat500J/kg·Ksourcebase material: wrought 316/316L (Cleveland-Cliffs), 0-100 °C580J/kg·Ksourcebase material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
Heats up and cools (diffusivity)4.1mm²/s1.59x faster2.59mm²/s
Thermal shock resistance2,067W/m4,825W/m2.33x more resistant
Melting pointnot sourced1,630–1,650°Csourcemelting range, wrought TIMETAL 6-4 (composition-level)
Values forEOS StainlessSteel 316L (powder 9011-0032), EOS M 290, ParameterSet 316L 20µm Surface M290/400W, as manufactured, horizontal; ISO 6892-1EOS Titanium Ti64ELI (powder 9011-0040; ASTM F136/F3001, i.e. Grade 23) on EOS M400 SF, parameter set Ti64ELI_030_FlexM400_100, 30 µm, as built; ISO 6892-1 A14

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS 316L Stainless Steel and DMLS Ti-6Al-4V ELI Titanium are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is DMLS 316L Stainless Steel stronger than DMLS Ti-6Al-4V ELI Titanium?

DMLS Ti-6Al-4V ELI Titanium is stronger: its yield strength is 1,100 MPa against 530 MPa for DMLS 316L Stainless Steel (2.08x).

Which is lighter, DMLS 316L Stainless Steel or DMLS Ti-6Al-4V ELI Titanium?

DMLS Ti-6Al-4V ELI Titanium is lighter: 4,400 kg/m³ against 7,900 kg/m³ for DMLS 316L Stainless Steel.

Which is stiffer, DMLS 316L Stainless Steel or DMLS Ti-6Al-4V ELI Titanium?

DMLS 316L Stainless Steel is stiffer: Young's modulus 185 GPa against 110 GPa for DMLS Ti-6Al-4V ELI Titanium, so the same part in DMLS 316L Stainless Steel deflects less under the same load.

Which is lighter for the same job, DMLS 316L Stainless Steel or DMLS Ti-6Al-4V ELI Titanium?

For the same stiffness or strength: DMLS Ti-6Al-4V ELI Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beDMLS 316L Stainless SteelDMLS Ti-6Al-4V ELI Titanium
Stiff rod or tie (tension)7% heavierlighter
Stiff beam (bending)38% heavierlighter
Stiff panel or plate1.51x heavierlighter
Strong rod or tie3.73x heavierlighter
Strong beam2.92x heavierlighter
Strong panel or plate2.59x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, DMLS 316L Stainless Steel or DMLS Ti-6Al-4V ELI Titanium?

DMLS 316L Stainless Steel conducts heat better: 16.2 W/m·K against 6.6 W/m·K for DMLS Ti-6Al-4V ELI Titanium.

Which expands less with temperature?

DMLS Ti-6Al-4V ELI Titanium expands less: 9 µm/m·K against 15.7 µm/m·K for DMLS 316L Stainless Steel.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS 316L Stainless SteelDMLS Ti-6Al-4V ELI Titanium
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS 316L Stainless SteelDMLS Ti-6Al-4V ELI Titanium
Strength against density