Materials / Compare

DMLS 17-4PH Stainless Steel vs. DMLS Ti-6Al-4V ELI Titanium

Compare DMLS 17-4PH Stainless Steel vs. DMLS Ti-6Al-4V ELI Titanium strength, stiffness, weight and thermal properties.

Change either side
DMLS 17-4PH Stainless Steel3D printed metal (DMLS)
DMLS Ti-6Al-4V ELI Titanium3D printed metal (DMLS)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength861MPasourcemean, as built, horizontal (N=72)1,100MPasourcetypical, as built, average of horizontal + vertical (M400)
Ultimate tensile strength886MPasourcemean, as built, horizontal (N=72)1,270MPasourcetypical, as built, average of horizontal + vertical (M400)
Elongation at break19.9%sourcemean at break, as built, horizontal8.7%sourcetypical at break, as built (M400)
Young's modulus (stiffness)197GPasourcebase material: wrought 17-4 PH, Condition H 900 (Cleveland-Cliffs)110GPasourcesame maker and process, sibling grade: EOS Titanium Ti64 (Grade 5) on EOS M 290, as built, XY and Z, typical
Density7,790kg/m³sourcemean part density (ISO 3369)4,400kg/m³sourcetypical part density (ISO 3369), M400
Strength to weight110kN·m/kg250kN·m/kg2.26x higher
Stiffness to weight25.3MN·m/kg1% higher25MN·m/kg
Poisson's ratio0.272sourcebase material: wrought 17-4 PH, all conditions (Cleveland-Cliffs)0.342sourcewrought TIMETAL 6-4 (TIMET measurement, mean of 10); composition-level, not DMLS-measured
Shear modulus77.4GPa1.89x stiffer in shear41GPa
Bulk modulus144GPa116GPa
Speed of sound5,029m/s5,000m/s
Thermal
Thermal conductivity17.9W/m·Ksourcebase material: wrought 17-4 PH, Condition H 900, at 149 °C (Cleveland-Cliffs)6.6W/m·Ksourcebase material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
Thermal expansion10.4µm/m·Ksourcemean 25-100 °C, ASTM E228, AFTER atmospheric heat treatment (as-built value not published)9µm/m·Ksourcemean 25-100 °C, ASTM E228; EOS Ti64 Grade 23 (=ELI) on EOS M 290 40 µm; condition not stated (sheet's mechanical data are heat treated)
100 mm part over a 50 °C swing52µm growth45µm growth16% less
Specific heat460J/kg·Ksourcebase material: wrought 17-4 PH, Condition A, 0-100 °C (Cleveland-Cliffs)580J/kg·Ksourcebase material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
Heats up and cools (diffusivity)5mm²/s1.93x faster2.59mm²/s
Thermal shock resistance5,474W/m13% more resistant4,825W/m
Melting pointnot sourced1,630–1,650°Csourcemelting range, wrought TIMETAL 6-4 (composition-level)
Values forEOS StainlessSteel 17-4PH IndustryLine (powder 9011-0041), EOS M 290, 40 µm, default job 17-4PH_040_StainlessM291_100, as built, horizontal; ISO 6892 & ASTM E8MEOS Titanium Ti64ELI (powder 9011-0040; ASTM F136/F3001, i.e. Grade 23) on EOS M400 SF, parameter set Ti64ELI_030_FlexM400_100, 30 µm, as built; ISO 6892-1 A14

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS 17-4PH Stainless Steel and DMLS Ti-6Al-4V ELI Titanium are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is DMLS 17-4PH Stainless Steel stronger than DMLS Ti-6Al-4V ELI Titanium?

DMLS Ti-6Al-4V ELI Titanium is stronger: its yield strength is 1,100 MPa against 861 MPa for DMLS 17-4PH Stainless Steel (28%).

Which is lighter, DMLS 17-4PH Stainless Steel or DMLS Ti-6Al-4V ELI Titanium?

DMLS Ti-6Al-4V ELI Titanium is lighter: 4,400 kg/m³ against 7,790 kg/m³ for DMLS 17-4PH Stainless Steel.

Which is stiffer, DMLS 17-4PH Stainless Steel or DMLS Ti-6Al-4V ELI Titanium?

DMLS 17-4PH Stainless Steel is stiffer: Young's modulus 197 GPa against 110 GPa for DMLS Ti-6Al-4V ELI Titanium, so the same part in DMLS 17-4PH Stainless Steel deflects less under the same load.

Which is lighter for the same job, DMLS 17-4PH Stainless Steel or DMLS Ti-6Al-4V ELI Titanium?

For the same stiffness or strength: DMLS 17-4PH Stainless Steel is lighter for a stiff rod or tie (tension); DMLS Ti-6Al-4V ELI Titanium is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beDMLS 17-4PH Stainless SteelDMLS Ti-6Al-4V ELI Titanium
Stiff rod or tie (tension)lighter1% heavier
Stiff beam (bending)32% heavierlighter
Stiff panel or plate46% heavierlighter
Strong rod or tie2.26x heavierlighter
Strong beam2.09x heavierlighter
Strong panel or plate2x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, DMLS 17-4PH Stainless Steel or DMLS Ti-6Al-4V ELI Titanium?

DMLS 17-4PH Stainless Steel conducts heat better: 17.9 W/m·K against 6.6 W/m·K for DMLS Ti-6Al-4V ELI Titanium.

Which expands less with temperature?

DMLS Ti-6Al-4V ELI Titanium expands less: 9 µm/m·K against 10.4 µm/m·K for DMLS 17-4PH Stainless Steel.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelDMLS Ti-6Al-4V ELI Titanium
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelBrickDMLS 17-4PH Stainless SteelDMLS Ti-6Al-4V ELI Titanium
Strength against density