Materials / DMLS

DMLS 17-4PH Stainless Steel

DMLS 17-4PH Stainless Steel strength, stiffness, density and thermal properties, with their source.

A bracket in DMLS 17-4PH Stainless Steel, as-sintered finish.

Process3D printed metal (DMLS)
Mechanical
Yield strength861MPasourcemean, as built, horizontal (N=72)
Ultimate tensile strength886MPasourcemean, as built, horizontal (N=72)
Elongation at break19.9%sourcemean at break, as built, horizontal
Young's modulus (stiffness)197GPasourcebase material: wrought 17-4 PH, Condition H 900 (Cleveland-Cliffs)
Density7,790kg/m³sourcemean part density (ISO 3369)
Strength to weight110kN·m/kg
Stiffness to weight25.3MN·m/kg
Poisson's ratio0.272sourcebase material: wrought 17-4 PH, all conditions (Cleveland-Cliffs)
Shear modulus77.4GPa
Bulk modulus144GPa
Speed of sound5,029m/s
Thermal
Thermal conductivity17.9W/m·Ksourcebase material: wrought 17-4 PH, Condition H 900, at 149 °C (Cleveland-Cliffs)
Thermal expansion10.4µm/m·Ksourcemean 25-100 °C, ASTM E228, AFTER atmospheric heat treatment (as-built value not published)
100 mm part over a 50 °C swing52µm growth
Specific heat460J/kg·Ksourcebase material: wrought 17-4 PH, Condition A, 0-100 °C (Cleveland-Cliffs)
Heats up and cools (diffusivity)5mm²/s
Thermal shock resistance5,474W/m
Values forEOS StainlessSteel 17-4PH IndustryLine (powder 9011-0041), EOS M 290, 40 µm, default job 17-4PH_040_StainlessM291_100, as built, horizontal; ISO 6892 & ASTM E8M

DMLS 17-4PH Stainless Steel is 3D printed: its properties depend on build direction and print settings; these are typical values.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless Steel
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelBrickDMLS 17-4PH Stainless Steel
Strength against density

Compare DMLS 17-4PH Stainless Steel with