DMLS 17-4PH Stainless Steel vs. Steel

Compare DMLS 17-4PH Stainless Steel vs. Steel strength, stiffness, weight and thermal properties.

Change either side
DMLS 17-4PH Stainless Steel3D printed metal (DMLS)
SteelWrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength861MPasourcemean, as built, horizontal (N=72)385MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISC
Ultimate tensile strength886MPasourcemean, as built, horizontal (N=72)505MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)
Elongation at break19.9%sourcemean at break, as built, horizontalnot sourced
Young's modulus (stiffness)197GPasourcebase material: wrought 17-4 PH, Condition H 900 (Cleveland-Cliffs)200GPasourcedesign value (AISC 360-16)
Density7,790kg/m³sourcemean part density (ISO 3369)7,850kg/m³sourcenominal (constructional data)
Strength to weight110kN·m/kg2.25x higher49kN·m/kg
Stiffness to weight25.3MN·m/kg25.5MN·m/kg
Poisson's ratio0.272sourcebase material: wrought 17-4 PH, all conditions (Cleveland-Cliffs)0.3sourcedesign value (AISC 360-16 Commentary)
Shear modulus77.4GPa76.9GPa
Bulk modulus144GPa167GPa
Speed of sound5,029m/s5,048m/s
Thermal
Thermal conductivity17.9W/m·Ksourcebase material: wrought 17-4 PH, Condition H 900, at 149 °C (Cleveland-Cliffs)48W/m·Ksourcenominal at 20 °C
Thermal expansion10.4µm/m·Ksourcemean 25-100 °C, ASTM E228, AFTER atmospheric heat treatment (as-built value not published)12µm/m·Ksourcenominal (constructional data, no temperature range stated)
100 mm part over a 50 °C swing52µm growth15% less60µm growth
Specific heat460J/kg·Ksourcebase material: wrought 17-4 PH, Condition A, 0-100 °C (Cleveland-Cliffs)460–480J/kg·Ksourcebase material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Heats up and cools (diffusivity)5mm²/s13mm²/s2.6x faster
Thermal shock resistance5,474W/m2% more resistant5,390W/m
Values forEOS StainlessSteel 17-4PH IndustryLine (powder 9011-0041), EOS M 290, 40 µm, default job 17-4PH_040_StainlessM291_100, as built, horizontal; ISO 6892 & ASTM E8MGeneric structural steel, cited as ASTM A992 (the current US structural grade): ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS 17-4PH Stainless Steel is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is DMLS 17-4PH Stainless Steel stronger than Steel?

DMLS 17-4PH Stainless Steel is stronger: its yield strength is 861 MPa against 385 MPa for Steel (2.24x).

Which is lighter, DMLS 17-4PH Stainless Steel or Steel?

DMLS 17-4PH Stainless Steel is lighter: 7,790 kg/m³ against 7,850 kg/m³ for Steel.

Which is stiffer, DMLS 17-4PH Stainless Steel or Steel?

Steel is stiffer: Young's modulus 200 GPa against 197 GPa for DMLS 17-4PH Stainless Steel, so the same part in Steel deflects less under the same load.

Which is lighter for the same job, DMLS 17-4PH Stainless Steel or Steel?

For the same stiffness or strength: DMLS 17-4PH Stainless Steel is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beDMLS 17-4PH Stainless SteelSteel
Stiff rod or tie (tension)about equalabout equal
Stiff beam (bending)about equalabout equal
Stiff panel or plateabout equalabout equal
Strong rod or tielighter2.25x heavier
Strong beamlighter1.72x heavier
Strong panel or platelighter1.51x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, DMLS 17-4PH Stainless Steel or Steel?

Steel conducts heat better: 48 W/m·K against 17.9 W/m·K for DMLS 17-4PH Stainless Steel.

Which expands less with temperature?

DMLS 17-4PH Stainless Steel expands less: 10.4 µm/m·K against 12 µm/m·K for Steel.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelSteel
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelBrickDMLS 17-4PH Stainless SteelSteel
Strength against density