Materials / Compare

Aluminum vs. Plastic PLA

Compare Aluminum vs. Plastic PLA strength, stiffness, weight and thermal properties.

AluminumWrought
Plastic PLA3D printed (FDM)
MechanicalAluminumPlastic PLA
Yield strength276MPa15.26x stronger52.5MPa2
Ultimate tensile strength310MPa15.9x stronger52.5MPa2
Flexural strengthnot sourced96.8MPa2
Elongation at break17%12.18x more ductile7.8%2
Young's modulus (stiffness)68.3GPa121x stiffer3.25GPa2
Density2,700kg/m³11,240kg/m³22.18x lighter
Strength to weight102kN·m/kg2.41x higher42.3kN·m/kg
Stiffness to weight25.3MN·m/kg9.65x higher2.62MN·m/kg
Poisson's ratio0.333not sourced
Shear modulus25.7GPanot sourced
Bulk modulus67GPanot sourced
Speed of sound5,030m/s3.11x faster1,619m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PETGPlastic ABSPlastic TPUPlastic NylonWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30AluminumPlastic PLA
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30AluminumPlastic PLA
Strength against densityHigher and further left: stronger for its weight
ThermalAluminumPlastic PLA
Thermal conductivity167W/m·K11,285x more heat through a finbase material0.13W/m·K4
Thermal expansion23.6µm/m·K1not sourced
100 mm part over a 50 °C swing118µm growthnot sourced
Specific heat896J/kg·K1base material1,200J/kg·K434% higher
Heats up and cools (diffusivity)69mm²/s790x faster0.0874mm²/s
Thermal shock resistance19,159W/mnot sourced
Melting pointsolidus-liquidus582–652°C1152°C2
Glass transitionnot sourced59.1°C2
Max service temperaturenot sourcedHDT 0.455 MPa58.8°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PETGPlastic ABSPlastic NylonRubberWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30AluminumPlastic PLA
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Kaiser Aluminum, UltiMaker, U.S. Department of Defense, NatureWorks
Aluminum
6061-T6/T651, Kaiser Aluminum typical properties (sheet, coil & plate datasheet); Poisson from MIL-HDBK-5J
Plastic PLA
Ultimaker PLA, 3D-printed specimens, XY (flat) orientation; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS dated April 20, 2022.
  1. 1
    Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum · Ultimate tensile strength: typicalAluminum · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum · Young's modulus (stiffness): typicalAluminum · Density: nominalAluminum · Thermal conductivity: typical, 20 °CAluminum · Thermal expansion: typical, mean 20-100 °CAluminum · Specific heat: typical, at 100 °CAluminum · Melting point: solidus-liquidus
  2. 2
    Ultimaker PLA Technical Data Sheet, v5.00UltiMakerarchived copyPlastic PLA · Yield strength: typicalPlastic PLA · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic PLA · Flexural strength: typicalPlastic PLA · Elongation at break: typicalPlastic PLA · Young's modulus (stiffness): typicalPlastic PLA · Density: typicalPlastic PLA · Melting point: typicalPlastic PLA · Glass transition: typicalPlastic PLA · Max service temperature: HDT 0.455 MPa (printed specimens)
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum · Poisson's ratio: typical (handbook physical constant)
  4. 4
    Engineering Properties of Ingeo BiopolymerNatureWorksarchived copyPlastic PLA · Thermal conductivity: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °CPlastic PLA · Specific heat: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PLA is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Aluminum stronger than Plastic PLA?

Aluminum is stronger: its yield strength is 276 MPa against 52.5 MPa for Plastic PLA (5.26x).

Which is lighter, Aluminum or Plastic PLA?

Plastic PLA is lighter: 1,240 kg/m³ against 2,700 kg/m³ for Aluminum.

Which is stiffer, Aluminum or Plastic PLA?

Aluminum is stiffer: Young's modulus 68.3 GPa against 3.25 GPa for Plastic PLA, so the same part in Aluminum deflects less under the same load.

Which is lighter for the same job, Aluminum or Plastic PLA?

For the same stiffness or strength: Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminumPlastic PLA
Stiff rod or tie (tension)lighter9.65x heavier
Stiff beam (bending)lighter2.11x heavier
Stiff panel or platelighter27% heavier
Strong rod or tielighter2.41x heavier
Strong beamlighter39% heavier
Strong panel or platelighter5% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum or Plastic PLA?

Aluminum stretches further before it breaks: 17% elongation at break against 7.8% for Plastic PLA.

Thermal

Which conducts heat better, Aluminum or Plastic PLA?

Aluminum conducts heat better: 167 W/m·K against 0.13 W/m·K for Plastic PLA.

Related comparisons