Materials / Compare

Brass C260 vs. DMLS Ti-6Al-4V ELI Titanium

Compare Brass C260 vs. DMLS Ti-6Al-4V ELI Titanium strength, stiffness, weight and thermal properties.

Brass C260Wrought
DMLS Ti-6Al-4V ELI Titanium3D printed metal (DMLS)
MechanicalBrass C260DMLS Ti-6Al-4V ELI Titanium
Yield strength345MPa11,100MPa23.19x stronger
Ultimate tensile strength427MPa11,270MPa22.97x stronger
Elongation at break23%12.64x more ductile8.7%2
Young's modulus (stiffness)110GPa3same maker and process110GPa4
Density8,525kg/m³34,400kg/m³21.94x lighter
Strength to weight40.5kN·m/kg250kN·m/kg6.18x higher
Stiffness to weight12.9MN·m/kg25MN·m/kg1.93x higher
Poisson's ratio0.345wrought TIMETAL 6-40.3426
Shear modulus41.2GPa41GPa
Bulk modulus115GPa116GPa
Speed of sound3,597m/s5,000m/s39% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260DMLS Ti-6Al-4V ELI Titanium
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260DMLS Ti-6Al-4V ELI Titanium
Strength against densityHigher and further left: stronger for its weight
ThermalBrass C260DMLS Ti-6Al-4V ELI Titanium
Thermal conductivity121W/m·K318.4x more heat through a finbase material6.6W/m·K7
Thermal expansion20µm/m·K3mean 25-100 °C9µm/m·K82.22x less
100 mm part over a 50 °C swing100µm growth45µm growth2.22x less
Specific heat377J/kg·K3base material580J/kg·K71.54x higher
Heats up and cools (diffusivity)37.7mm²/s14.6x faster2.59mm²/s
Thermal shock resistance12,510W/m2.59x more resistant4,825W/m
Melting pointsolidus-liquidus916–954°C3melting range1,630–1,650°C6
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260DMLS Ti-6Al-4V ELI Titanium
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260DMLS Ti-6Al-4V ELI Titanium
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources8 documents: Copper Development Association, EOS GmbH, Wieland, TIMET
Brass C260
C26000 cartridge brass, H02 half hard flat/strip: CDA Electronic Connector Design Guide (mechanical) + CDA alloy page (physical)
DMLS Ti-6Al-4V ELI Titanium
EOS Titanium Ti64ELI (powder 9011-0040; ASTM F136/F3001, i.e. Grade 23) on EOS M400 SF, parameter set Ti64ELI_030_FlexM400_100, 30 µm, as built; ISO 6892-1 A14
  1. 1
    Electronic Connector Design Guide: Cold Rolled TempersCopper Development Associationarchived copyBrass C260 · Yield strength: nominal, strip/flat, 0.5% extension (not 0.2% offset)Brass C260 · Ultimate tensile strength: nominal, strip/flatBrass C260 · Elongation at break: nominal, in 2.0 in., strip/flat
  2. 2
    EOS Titanium Ti64ELI Material Data Sheet, M 290 and M 400EOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Yield strength: typical, as built, average of horizontal + vertical (M400)DMLS Ti-6Al-4V ELI Titanium · Ultimate tensile strength: typical, as built, average of horizontal + vertical (M400)DMLS Ti-6Al-4V ELI Titanium · Elongation at break: typical at break, as built (M400)DMLS Ti-6Al-4V ELI Titanium · Density: typical part density (ISO 3369), M400
  3. 3
    C26000 Alloy (copper.org)Copper Development Associationarchived copyBrass C260 · Young's modulus (stiffness): typical, temper-independentBrass C260 · Density: nominalBrass C260 · Thermal conductivity: typical, 20 °CBrass C260 · Thermal expansion: typical, mean 20-300 °CBrass C260 · Specific heat: typical, 20 °CBrass C260 · Melting point: solidus-liquidus
  4. 4
    EOS Titanium Ti64 Material Data Sheet, M 290 (2022)EOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Young's modulus (stiffness): same maker and process, sibling grade: EOS Titanium Ti64 (Grade 5) on EOS M 290, as built, XY and Z, typical
  5. 5
    Wieland-M30 (CuZn30, C26000) Data SheetWielandarchived copyBrass C260 · Poisson's ratio: reference value at room temperature (Wieland-M30 = CuZn30 = C26000, rolled products)
  6. 6
    TIMETAL 6-4 PropertiesTIMETarchived copyDMLS Ti-6Al-4V ELI Titanium · Poisson's ratio: wrought TIMETAL 6-4 (TIMET measurement, mean of 10); composition-level, not DMLS-measuredDMLS Ti-6Al-4V ELI Titanium · Melting point: melting range, wrought TIMETAL 6-4 (composition-level)
  7. 7
    TIMETAL 6-4 Data SheetTIMETarchived copyDMLS Ti-6Al-4V ELI Titanium · Thermal conductivity: base material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °CDMLS Ti-6Al-4V ELI Titanium · Specific heat: base material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
  8. 8
    EOS Titanium Ti64 Grade 23 Material Data SheetEOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Thermal expansion: mean 25-100 °C, ASTM E228; EOS Ti64 Grade 23 (=ELI) on EOS M 290 40 µm; condition not stated (sheet's mechanical data are heat treated)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS Ti-6Al-4V ELI Titanium is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Brass C260 stronger than DMLS Ti-6Al-4V ELI Titanium?

DMLS Ti-6Al-4V ELI Titanium is stronger: its yield strength is 1,100 MPa against 345 MPa for Brass C260 (3.19x).

Which is lighter, Brass C260 or DMLS Ti-6Al-4V ELI Titanium?

DMLS Ti-6Al-4V ELI Titanium is lighter: 4,400 kg/m³ against 8,525 kg/m³ for Brass C260.

Which is stiffer, Brass C260 or DMLS Ti-6Al-4V ELI Titanium?

Brass C260 is stiffer: Young's modulus 110 GPa against 110 GPa for DMLS Ti-6Al-4V ELI Titanium, so the same part in Brass C260 deflects less under the same load.

Which is lighter for the same job, Brass C260 or DMLS Ti-6Al-4V ELI Titanium?

For the same stiffness or strength: DMLS Ti-6Al-4V ELI Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beBrass C260DMLS Ti-6Al-4V ELI Titanium
Stiff rod or tie (tension)1.93x heavierlighter
Stiff beam (bending)1.93x heavierlighter
Stiff panel or plate1.94x heavierlighter
Strong rod or tie6.18x heavierlighter
Strong beam4.2x heavierlighter
Strong panel or plate3.46x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Brass C260 or DMLS Ti-6Al-4V ELI Titanium?

Brass C260 stretches further before it breaks: 23% elongation at break against 8.7% for DMLS Ti-6Al-4V ELI Titanium.

Thermal

Which conducts heat better, Brass C260 or DMLS Ti-6Al-4V ELI Titanium?

Brass C260 conducts heat better: 121 W/m·K against 6.6 W/m·K for DMLS Ti-6Al-4V ELI Titanium.

Which expands less with temperature?

DMLS Ti-6Al-4V ELI Titanium expands less: 9 µm/m·K against 20 µm/m·K for Brass C260.

Related comparisons