Materials / Compare

Brass C260 vs. SLA Resin Tough 2000

Compare Brass C260 vs. SLA Resin Tough 2000 strength, stiffness, weight and thermal properties.

Brass C260Wrought
SLA Resin Tough 20003D printed (SLA resin)
MechanicalBrass C260SLA Resin Tough 2000
Yield strength345MPa18.54x stronger40.4MPa2
Ultimate tensile strength427MPa110.6x stronger40.4MPa2
Flexural strengthnot sourced67MPa2
Elongation at break23%179%23.43x more ductile
Young's modulus (stiffness)110GPa361.3x stiffer1.8GPa2
Density8,525kg/m³31,090kg/m³27.82x lighter
Strength to weight40.5kN·m/kg9% higher37.1kN·m/kg
Stiffness to weight12.9MN·m/kg7.83x higher1.65MN·m/kg
Poisson's ratio0.344not sourced
Shear modulus41.2GPanot sourced
Bulk modulus115GPanot sourced
Speed of sound3,597m/s2.8x faster1,285m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260SLA Resin Tough 2000
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260SLA Resin Tough 2000
Strength against densityHigher and further left: stronger for its weight
ThermalBrass C260SLA Resin Tough 2000
Thermal conductivity121W/m·K3not sourced
Thermal expansion20µm/m·K36.71x lessmean 0-150 °C134µm/m·K2
100 mm part over a 50 °C swing100µm growth6.71x less671µm growth
Specific heat377J/kg·K3not sourced
Heats up and cools (diffusivity)37.7mm²/snot sourced
Thermal shock resistance12,510W/mnot sourced
Melting pointsolidus-liquidus916–954°C3not sourced
Glass transitionnot sourcedDMA112°C2
Max service temperaturenot sourcedHDT 1.8 MPa57°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Copper Development Association, Formlabs, Wieland
Brass C260
C26000 cartridge brass, H02 half hard flat/strip: CDA Electronic Connector Design Guide (mechanical) + CDA alloy page (physical)
SLA Resin Tough 2000
Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.
  1. 1
    Electronic Connector Design Guide: Cold Rolled TempersCopper Development Associationarchived copyBrass C260 · Yield strength: nominal, strip/flat, 0.5% extension (not 0.2% offset)Brass C260 · Ultimate tensile strength: nominal, strip/flatBrass C260 · Elongation at break: nominal, in 2.0 in., strip/flat
  2. 2
    Tough 2000 Resin V2 Technical Data Sheet (2025)Formlabsarchived copySLA Resin Tough 2000 · Yield strength: typicalSLA Resin Tough 2000 · Ultimate tensile strength: typicalSLA Resin Tough 2000 · Flexural strength: typicalSLA Resin Tough 2000 · Elongation at break: typicalSLA Resin Tough 2000 · Young's modulus (stiffness): typicalSLA Resin Tough 2000 · Density: typicalSLA Resin Tough 2000 · Thermal expansion: mean 0-150 °CSLA Resin Tough 2000 · Glass transition: DMASLA Resin Tough 2000 · Max service temperature: HDT 1.8 MPa
  3. 3
    C26000 Alloy (copper.org)Copper Development Associationarchived copyBrass C260 · Young's modulus (stiffness): typical, temper-independentBrass C260 · Density: nominalBrass C260 · Thermal conductivity: typical, 20 °CBrass C260 · Thermal expansion: typical, mean 20-300 °CBrass C260 · Specific heat: typical, 20 °CBrass C260 · Melting point: solidus-liquidus
  4. 4
    Wieland-M30 (CuZn30, C26000) Data SheetWielandarchived copyBrass C260 · Poisson's ratio: reference value at room temperature (Wieland-M30 = CuZn30 = C26000, rolled products)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Brass C260 stronger than SLA Resin Tough 2000?

Brass C260 is stronger: its yield strength is 345 MPa against 40.4 MPa for SLA Resin Tough 2000 (8.54x).

Which is lighter, Brass C260 or SLA Resin Tough 2000?

SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 8,525 kg/m³ for Brass C260.

Which is stiffer, Brass C260 or SLA Resin Tough 2000?

Brass C260 is stiffer: Young's modulus 110 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Brass C260 deflects less under the same load.

Which is lighter for the same job, Brass C260 or SLA Resin Tough 2000?

For the same stiffness or strength: Brass C260 is lighter for a stiff rod or tie (tension), strong rod or tie; SLA Resin Tough 2000 is lighter for a stiff panel or plate, strong beam, strong panel or plate.

Part that must beBrass C260SLA Resin Tough 2000
Stiff rod or tie (tension)lighter7.83x heavier
Stiff beam (bending)about equalabout equal
Stiff panel or plate1.98x heavierlighter
Strong rod or tielighter9% heavier
Strong beam1.87x heavierlighter
Strong panel or plate2.68x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Brass C260 or SLA Resin Tough 2000?

SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 23% for Brass C260.

Thermal

Which expands less with temperature?

Brass C260 expands less: 20 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.

Related comparisons