Materials / Compare

Brass C360 vs. Ceramic Aluminum Nitride

Compare Brass C360 vs. Ceramic Aluminum Nitride strength, stiffness, weight and thermal properties.

Brass C360Wrought
Ceramic Aluminum NitrideSintered ceramic (pressed and fired)
MechanicalBrass C360Ceramic Aluminum Nitride
Yield strength310MPa1none (brittle)
Ultimate tensile strength400MPa1not sourced
Flexural strengthnot sourced310MPa2
Elongation at break25%1none (brittle)
Young's modulus (stiffness)96.5GPa1320GPa23.32x stiffer
Density8,498kg/m³13,400kg/m³22.5x lighter
Strength to weight36.5kN·m/kgnot sourced
Stiffness to weight11.4MN·m/kg94.1MN·m/kg8.29x higher
Poisson's ratiobase material0.3430.242
Shear modulus36GPa129GPa3.58x stiffer in shear
Bulk modulus101GPa205GPa2.04x higher
Speed of sound3,370m/s9,701m/s2.88x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360Ceramic Aluminum Nitride
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360
Strength against densityHigher and further left: stronger for its weight
ThermalBrass C360Ceramic Aluminum Nitride
Thermal conductivity116W/m·K1150W/m·K229% more heat through a fin
Thermal expansion20.5µm/m·K1mean4.6µm/m·K24.46x less
100 mm part over a 50 °C swing103µm growth23µm growth4.46x less
Specific heat377J/kg·K1710J/kg·K21.88x higher
Heats up and cools (diffusivity)36.2mm²/s62.1mm²/s1.72x faster
Thermal shock resistance11,997W/mnot sourced
Melting pointsolidus-liquidus888–899°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360Ceramic Aluminum Nitride
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360Ceramic Aluminum Nitride
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Copper Development Association, KYOCERA Fineceramics Europe, Wieland
Brass C360
C36000 free-cutting brass, H02 half-hard rod 1 in. section (20% cold work), copper.org typical values
Ceramic Aluminum Nitride
KYOCERA AN216A dense sintered aluminium nitride, typical values; KYOCERA Fineceramics Europe data sheet 2023.04.03
  1. 1
    C36000 Alloy (copper.org)Copper Development Associationarchived copyBrass C360 · Yield strength: typical, 0.5% extension under loadBrass C360 · Ultimate tensile strength: typicalBrass C360 · Elongation at break: typical, 1 in. rodBrass C360 · Young's modulus (stiffness): typical, temper-independentBrass C360 · Density: nominalBrass C360 · Thermal conductivity: typical, 20 °CBrass C360 · Thermal expansion: typical, mean 20-300 °CBrass C360 · Specific heat: typical, 20 °CBrass C360 · Melting point: solidus-liquidus
  2. 2
    AN216A Aluminium Nitride Data Sheet (2023)KYOCERA Fineceramics Europearchived copyCeramic Aluminum Nitride · Flexural strength: 3-point bending strength (JIS R 1601)Ceramic Aluminum Nitride · Young's modulus (stiffness): typical (JIS R 1602)Ceramic Aluminum Nitride · Density: typical (JIS R 1634)Ceramic Aluminum Nitride · Poisson's ratio: typical (JIS R 1602)Ceramic Aluminum Nitride · Thermal conductivity: typical (JIS R 1611)Ceramic Aluminum Nitride · Thermal expansion: mean, 40-400 °C (JIS R 1618)Ceramic Aluminum Nitride · Specific heat: typical (JIS R 1611)
  3. 3
    Wieland-Z30 (CuZn39Pb2, C37700) Data SheetWielandarchived copyBrass C360 · Poisson's ratio: base material: leaded free-machining brass CuZn39Pb2 (C37700), Wieland-Z30 rolled products, reference value at room temperature

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Which is lighter, Brass C360 or Ceramic Aluminum Nitride?

Ceramic Aluminum Nitride is lighter: 3,400 kg/m³ against 8,498 kg/m³ for Brass C360.

Which is stiffer, Brass C360 or Ceramic Aluminum Nitride?

Ceramic Aluminum Nitride is stiffer: Young's modulus 320 GPa against 96.5 GPa for Brass C360, so the same part in Ceramic Aluminum Nitride deflects less under the same load.

Which is lighter for the same job, Brass C360 or Ceramic Aluminum Nitride?

For the same stiffness or strength: Ceramic Aluminum Nitride is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beBrass C360Ceramic Aluminum Nitride
Stiff rod or tie (tension)8.29x heavierlighter
Stiff beam (bending)4.55x heavierlighter
Stiff panel or plate3.73x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Brass C360 or Ceramic Aluminum Nitride?

Ceramic Aluminum Nitride conducts heat better: 150 W/m·K against 116 W/m·K for Brass C360.

Which expands less with temperature?

Ceramic Aluminum Nitride expands less: 4.6 µm/m·K against 20.5 µm/m·K for Brass C360.

Related comparisons