Materials / Compare

Ceramic Alumina 96% vs. Plastic PBT GF30

Compare Ceramic Alumina 96% vs. Plastic PBT GF30 strength, stiffness, weight and thermal properties.

Ceramic Alumina 96%Sintered ceramic (pressed and fired)
Plastic PBT GF30Bulk polymer (molded or machined)
MechanicalCeramic Alumina 96%Plastic PBT GF30
Yield strengthnone (brittle)not given (tensile used)
Ultimate tensile strength221MPa1stress at break140MPa2
Compressive strength2,068MPa1not sourced
Flexural strengthflexural strength358MPa1210MPa2
Elongation at breaknone (brittle)strain at break3%2
Young's modulus (stiffness)303GPa130.9x stiffer9.8GPa2
Density3,720kg/m³11,530kg/m³22.43x lighter
Strength to weight59.4kN·m/kg91.5kN·m/kg1.54x higher
Stiffness to weight81.5MN·m/kg12.7x higher6.41MN·m/kg
Poisson's ratio0.211not sourced
Shear modulus125GPanot sourced
Bulk modulus174GPanot sourced
Speed of sound9,025m/s3.57x faster2,531m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%Plastic PBT GF30
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%Plastic PBT GF30
Strength against densityHigher and further left: stronger for its weight
ThermalCeramic Alumina 96%Plastic PBT GF30
Thermal conductivity24.7W/m·K191.5x more heat through a fin0.27W/m·K2
Thermal expansionmean8.2µm/m·K13.05x lesslongitudinal25µm/m·K2
100 mm part over a 50 °C swing41µm growth3.05x less125µm growth
Specific heat880J/kg·K11,050J/kg·K219% higher
Heats up and cools (diffusivity)7.55mm²/s44.9x faster0.168mm²/s
Thermal shock resistance1,736W/mnot sourced
Melting pointnot sourcedDSC223°C2
Max service temperaturenot sourcedHDT 1.8 MPa205°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%Plastic PBT GF30
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%Plastic PBT GF30
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources2 documents: CoorsTek, BASF
Ceramic Alumina 96%
CoorsTek AD-96, nominal 96% Al2O3 sintered alumina, typical values; CoorsTek "Ceramic Seal Material Properties" (© 2018, 01899 F). AD-96 is the general 96% grade, not the ADS-96R substrate grade.
Plastic PBT GF30
BASF Ultradur B 4300 G6 (PBT, 30% glass fibre), injection moulding grade; product information sheet 09/2026, typical values for uncoloured product at 23 °C.
  1. 1
    Ceramic Seal Material Properties (01899 F)CoorsTekarchived copyCeramic Alumina 96% · Ultimate tensile strength: typical tensile strength, 25 °C (ACMA Test #4)Ceramic Alumina 96% · Compressive strength: typical, 20 °C (ASTM-C773)Ceramic Alumina 96% · Flexural strength: flexural strength (MOR), 20 °C (ASTM-F417)Ceramic Alumina 96% · Young's modulus (stiffness): typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Density: typical (ASTM-C20)Ceramic Alumina 96% · Poisson's ratio: typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Thermal conductivity: typical, 20 °C (ASTM-C408)Ceramic Alumina 96% · Thermal expansion: mean, 25-1000 °C (ASTM-C372)Ceramic Alumina 96% · Specific heat: typical, 100 °C (ASTM-E1269)
  2. 2
    Ultradur B 4300 G6 Product InformationBASFPlastic PBT GF30 · Ultimate tensile strength: stress at break, 23 °CPlastic PBT GF30 · Flexural strength: typical, 23 °CPlastic PBT GF30 · Elongation at break: strain at break, 23 °CPlastic PBT GF30 · Young's modulus (stiffness): typical, 23 °CPlastic PBT GF30 · Density: typicalPlastic PBT GF30 · Thermal conductivity: typical (DIN 52612-1)Plastic PBT GF30 · Thermal expansion: longitudinal (flow), mean 23-55 °CPlastic PBT GF30 · Specific heat: typical, 23 °CPlastic PBT GF30 · Melting point: DSC (ISO 11357)Plastic PBT GF30 · Max service temperature: HDT 1.8 MPa

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Ceramic Alumina 96% stronger than Plastic PBT GF30?

Ceramic Alumina 96% is stronger: its tensile strength is 221 MPa against 140 MPa for Plastic PBT GF30 (1.58x).

Which is lighter, Ceramic Alumina 96% or Plastic PBT GF30?

Plastic PBT GF30 is lighter: 1,530 kg/m³ against 3,720 kg/m³ for Ceramic Alumina 96%.

Which is stiffer, Ceramic Alumina 96% or Plastic PBT GF30?

Ceramic Alumina 96% is stiffer: Young's modulus 303 GPa against 9.8 GPa for Plastic PBT GF30, so the same part in Ceramic Alumina 96% deflects less under the same load.

Which is lighter for the same job, Ceramic Alumina 96% or Plastic PBT GF30?

For the same stiffness or strength: Ceramic Alumina 96% is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Plastic PBT GF30 is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beCeramic Alumina 96%Plastic PBT GF30
Stiff rod or tie (tension)lighter12.7x heavier
Stiff beam (bending)lighter2.29x heavier
Stiff panel or platelighter29% heavier
Strong rod or tie1.54x heavierlighter
Strong beam1.79x heavierlighter
Strong panel or plate1.94x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Ceramic Alumina 96% or Plastic PBT GF30?

Ceramic Alumina 96% conducts heat better: 24.7 W/m·K against 0.27 W/m·K for Plastic PBT GF30.

Which expands less with temperature?

Ceramic Alumina 96% expands less: 8.2 µm/m·K against 25 µm/m·K for Plastic PBT GF30.

Related comparisons