Materials / Compare

Ceramic Alumina 96% vs. Steel

Compare Ceramic Alumina 96% vs. Steel strength, stiffness, weight and thermal properties.

Change either side
Ceramic Alumina 96%Sintered ceramic (pressed and fired)
SteelWrought
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)385MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISC
Ultimate tensile strength221MPasourcetypical tensile strength, 25 °C (ACMA Test #4)505MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)
Compressive strength2,068MPasourcetypical, 20 °C (ASTM-C773)not sourced
Flexural strength358MPasourceflexural strength (MOR), 20 °C (ASTM-F417)not sourced
Elongation at breaknot sourcednot sourced
Young's modulus (stiffness)303GPasourcetypical, 20 °C (ASTM-C848)200GPasourcedesign value (AISC 360-16)
Density3,720kg/m³sourcetypical (ASTM-C20)7,850kg/m³sourcenominal (constructional data)
Strength to weight59.4kN·m/kg21% higher49kN·m/kg
Stiffness to weight81.5MN·m/kg3.2x higher25.5MN·m/kg
Poisson's ratio0.21sourcetypical, 20 °C (ASTM-C848)0.3sourcedesign value (AISC 360-16 Commentary)
Shear modulus125GPa1.63x stiffer in shear76.9GPa
Bulk modulus174GPa167GPa
Speed of sound9,025m/s5,048m/s
Thermal
Thermal conductivity24.7W/m·Ksourcetypical, 20 °C (ASTM-C408)48W/m·Ksourcenominal at 20 °C
Thermal expansion8.2µm/m·Ksourcemean, 25-1000 °C (ASTM-C372)12µm/m·Ksourcenominal (constructional data, no temperature range stated)
100 mm part over a 50 °C swing41µm growth46% less60µm growth
Specific heat880J/kg·Ksourcetypical, 100 °C (ASTM-E1269)460–480J/kg·Ksourcebase material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Heats up and cools (diffusivity)7.55mm²/s13mm²/s1.72x faster
Thermal shock resistance1,736W/m5,390W/m3.11x more resistant
Values forCoorsTek AD-96, nominal 96% Al2O3 sintered alumina, typical values; CoorsTek "Ceramic Seal Material Properties" (© 2018, 01899 F). AD-96 is the general 96% grade, not the ADS-96R substrate grade.Generic structural steel, cited as ASTM A992 (the current US structural grade): ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Ceramic Alumina 96% stronger than Steel?

Steel is stronger: its yield strength is 385 MPa against tensile strength 221 MPa for Ceramic Alumina 96% (1.74x).

Which is lighter, Ceramic Alumina 96% or Steel?

Ceramic Alumina 96% is lighter: 3,720 kg/m³ against 7,850 kg/m³ for Steel.

Which is stiffer, Ceramic Alumina 96% or Steel?

Ceramic Alumina 96% is stiffer: Young's modulus 303 GPa against 200 GPa for Steel, so the same part in Ceramic Alumina 96% deflects less under the same load.

Which is lighter for the same job, Ceramic Alumina 96% or Steel?

For the same stiffness or strength: Ceramic Alumina 96% is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beCeramic Alumina 96%Steel
Stiff rod or tie (tension)lighter3.2x heavier
Stiff beam (bending)lighter2.6x heavier
Stiff panel or platelighter2.42x heavier
Strong rod or tielighter21% heavier
Strong beamlighter46% heavier
Strong panel or platelighter1.6x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Ceramic Alumina 96% or Steel?

Steel conducts heat better: 48 W/m·K against 24.7 W/m·K for Ceramic Alumina 96%.

Which expands less with temperature?

Ceramic Alumina 96% expands less: 8.2 µm/m·K against 12 µm/m·K for Steel.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%Steel
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%Steel
Strength against density