Materials / Compare

Ceramic Aluminum Nitride vs. Magnesium AZ31B-H24

Compare Ceramic Aluminum Nitride vs. Magnesium AZ31B-H24 strength, stiffness, weight and thermal properties.

Ceramic Aluminum NitrideSintered ceramic (pressed and fired)
Magnesium AZ31B-H24Wrought
MechanicalCeramic Aluminum NitrideMagnesium AZ31B-H24
Yield strengthnone (brittle)220MPa1
Ultimate tensile strengthnot sourced290MPa1
Flexural strength310MPa2not sourced
Elongation at breaknone (brittle)13%1
Young's modulus (stiffness)320GPa27.14x stiffer44.8GPa3
Density3,400kg/m³21,769kg/m³31.92x lighter
Strength to weightnot sourced124kN·m/kg
Stiffness to weight94.1MN·m/kg3.72x higher25.3MN·m/kg
Poisson's ratio0.2420.353
Shear modulus129GPa7.78x stiffer in shear16.6GPa
Bulk modulus205GPa4.12x higher49.8GPa
Speed of sound9,701m/s1.93x faster5,032m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Aluminum NitrideMagnesium AZ31B-H24
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Magnesium AZ31B-H24
Strength against densityHigher and further left: stronger for its weight
ThermalCeramic Aluminum NitrideMagnesium AZ31B-H24
Thermal conductivity150W/m·K21.95x more heat through a fin76.9W/m·K1
Thermal expansionmean4.6µm/m·K25.83x less26.8µm/m·K1
100 mm part over a 50 °C swing23µm growth5.83x less134µm growth
Specific heat710J/kg·K21,040J/kg·K146% higher
Heats up and cools (diffusivity)62.1mm²/s49% faster41.8mm²/s
Thermal shock resistancenot sourced9,159W/m
Max service temperaturenot sourced149°C3
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Aluminum NitrideMagnesium AZ31B-H24
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Aluminum NitrideMagnesium AZ31B-H24
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Magnesium Elektron, KYOCERA Fineceramics Europe, U.S. Department of Defense
Ceramic Aluminum Nitride
KYOCERA AN216A dense sintered aluminium nitride, typical values; KYOCERA Fineceramics Europe data sheet 2023.04.03
Magnesium AZ31B-H24
AZ31B-H24 sheet 0.016-0.062 in., MIL-HDBK-5J Table 4.2.1.0(b) (AMS 4377); strengths are S-basis MINIMUMS
  1. 1
    Elektron AZ31B Sheet, Plate & Coil (Datasheet 482)Magnesium Elektronarchived copyMagnesium AZ31B-H24 · Yield strength: typical, H24, 0.5-6 mm, 0.2 % proof stressMagnesium AZ31B-H24 · Ultimate tensile strength: typical, H24, 0.5-6 mmMagnesium AZ31B-H24 · Elongation at break: typical, H24, 0.5-6 mm, gauge 5.65√AMagnesium AZ31B-H24 · Thermal conductivity: typical (temper/temperature not stated)Magnesium AZ31B-H24 · Thermal expansion: typical (temperature range not stated)Magnesium AZ31B-H24 · Specific heat: typical
  2. 2
    AN216A Aluminium Nitride Data Sheet (2023)KYOCERA Fineceramics Europearchived copyCeramic Aluminum Nitride · Flexural strength: 3-point bending strength (JIS R 1601)Ceramic Aluminum Nitride · Young's modulus (stiffness): typical (JIS R 1602)Ceramic Aluminum Nitride · Density: typical (JIS R 1634)Ceramic Aluminum Nitride · Poisson's ratio: typical (JIS R 1602)Ceramic Aluminum Nitride · Thermal conductivity: typical (JIS R 1611)Ceramic Aluminum Nitride · Thermal expansion: mean, 40-400 °C (JIS R 1618)Ceramic Aluminum Nitride · Specific heat: typical (JIS R 1611)
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ31B-H24 · Young's modulus (stiffness): typical (handbook physical constant)Magnesium AZ31B-H24 · Density: nominalMagnesium AZ31B-H24 · Poisson's ratio: typical (handbook physical constant)Magnesium AZ31B-H24 · Max service temperature: stated application limit

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Which is lighter, Ceramic Aluminum Nitride or Magnesium AZ31B-H24?

Magnesium AZ31B-H24 is lighter: 1,769 kg/m³ against 3,400 kg/m³ for Ceramic Aluminum Nitride.

Which is stiffer, Ceramic Aluminum Nitride or Magnesium AZ31B-H24?

Ceramic Aluminum Nitride is stiffer: Young's modulus 320 GPa against 44.8 GPa for Magnesium AZ31B-H24, so the same part in Ceramic Aluminum Nitride deflects less under the same load.

Which is lighter for the same job, Ceramic Aluminum Nitride or Magnesium AZ31B-H24?

For the same stiffness or strength: Ceramic Aluminum Nitride is lighter for a stiff rod or tie (tension), stiff beam (bending).

Part that must beCeramic Aluminum NitrideMagnesium AZ31B-H24
Stiff rod or tie (tension)lighter3.72x heavier
Stiff beam (bending)lighter39% heavier
Stiff panel or plateabout equalabout equal

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Ceramic Aluminum Nitride or Magnesium AZ31B-H24?

Ceramic Aluminum Nitride conducts heat better: 150 W/m·K against 76.9 W/m·K for Magnesium AZ31B-H24.

Which expands less with temperature?

Ceramic Aluminum Nitride expands less: 4.6 µm/m·K against 26.8 µm/m·K for Magnesium AZ31B-H24.