Materials / Compare
Concrete vs. DMLS Ti-6Al-4V ELI Titanium
Compare Concrete vs. DMLS Ti-6Al-4V ELI Titanium strength, stiffness, weight and thermal properties.
| Mechanical | Concrete | DMLS Ti-6Al-4V ELI Titanium |
|---|---|---|
| Yield strength | none (brittle) | 1,100MPa1 |
| Ultimate tensile strength | not sourced | 1,270MPa1 |
| Compressive strength | 27.6MPa2 | not sourced |
| Elongation at break | none (brittle) | 8.7%1 |
| Young's modulus (stiffness) | design value25.1GPa3 | same maker and process110GPa4 |
| Density | 2,240–2,400kg/m³5 | 4,400kg/m³1 |
| Strength to weight | not sourced | 250kN·m/kg |
| Stiffness to weight | 10.8MN·m/kg | 25MN·m/kg2.31x higher |
| Poisson's ratio | 0.15–0.26 | wrought TIMETAL 6-40.3427 |
| Shear modulus | 10.7GPa | 41GPa3.84x stiffer in shear |
| Bulk modulus | 12.9GPa | 116GPa9.01x higher |
| Speed of sound | 3,289m/s | 5,000m/s1.52x faster |
| Thermal | Concrete | DMLS Ti-6Al-4V ELI Titanium |
|---|---|---|
| Thermal conductivity | 0.9W/m·K8 | base material6.6W/m·K97.33x more heat through a fin |
| Thermal expansion | 8–12µm/m·K10 | mean 25-100 °C9µm/m·K11 |
| 100 mm part over a 50 °C swing | 50µm growth | 45µm growth11% less |
| Specific heat | 900J/kg·K121.55x higher | base material580J/kg·K9 |
| Heats up and cools (diffusivity) | 0.431mm²/s | 2.59mm²/s6x faster |
| Thermal shock resistance | not sourced | 4,825W/m |
| Melting point | not sourced | melting range1,630–1,650°C7 |
| Max service temperature | 65°C6 | not sourced |
| Try it on a partA sample part to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources12 documents: EOS GmbH, National Ready Mixed Concrete Association, Federal Highway Administration, Oak Ridge National Laboratory, TIMET, USDA Forest Products Laboratory, National Institute of Standards and Technology
- Concrete
- Normal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC review
- DMLS Ti-6Al-4V ELI Titanium
- EOS Titanium Ti64ELI (powder 9011-0040; ASTM F136/F3001, i.e. Grade 23) on EOS M400 SF, parameter set Ti64ELI_030_FlexM400_100, 30 µm, as built; ISO 6892-1 A14
- 1EOS Titanium Ti64ELI Material Data Sheet, M 290 and M 400EOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Yield strength: typical, as built, average of horizontal + vertical (M400)DMLS Ti-6Al-4V ELI Titanium · Ultimate tensile strength: typical, as built, average of horizontal + vertical (M400)DMLS Ti-6Al-4V ELI Titanium · Elongation at break: typical at break, as built (M400)DMLS Ti-6Al-4V ELI Titanium · Density: typical part density (ISO 3369), M400
- 2CIP 35: Testing Compressive Strength of ConcreteNational Ready Mixed Concrete Associationarchived copyConcrete · Compressive strength: specified compressive strength class (f'c), not a measured typical
- 3LRFD Steel Girder Superstructure Bridge Design Example, Design Step 2: Concrete Deck DesignFederal Highway AdministrationConcrete · Young's modulus (stiffness): design value: AASHTO LRFD 5.4.2.4 applied by FHWA to f'c = 4.0 ksi normal-weight concrete
- 4EOS Titanium Ti64 Material Data Sheet, M 290 (2022)EOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Young's modulus (stiffness): same maker and process, sibling grade: EOS Titanium Ti64 (Grade 5) on EOS M 290, as built, XY and Z, typical
- 5CIP 36: Structural Lightweight ConcreteNational Ready Mixed Concrete Associationarchived copyConcrete · Density: range for normalweight concrete
- 6The Effect of Elevated Temperature on Concrete Materials and Structures: A Literature Review (ORNL/TM-2005/553)Oak Ridge National Laboratoryarchived copyConcrete · Poisson's ratio: general range at normal ambient conditions (overall 0.11-0.32)Concrete · Max service temperature: code long-term temperature limit (ASME Code, concrete containments)
- 7TIMETAL 6-4 PropertiesTIMETarchived copyDMLS Ti-6Al-4V ELI Titanium · Poisson's ratio: wrought TIMETAL 6-4 (TIMET measurement, mean of 10); composition-level, not DMLS-measuredDMLS Ti-6Al-4V ELI Titanium · Melting point: melting range, wrought TIMETAL 6-4 (composition-level)
- 8Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of WoodUSDA Forest Products LaboratoryConcrete · Thermal conductivity: typical (comparative value)
- 9TIMETAL 6-4 Data SheetTIMETarchived copyDMLS Ti-6Al-4V ELI Titanium · Thermal conductivity: base material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °CDMLS Ti-6Al-4V ELI Titanium · Specific heat: base material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
- 10Thermal Coefficient of Portland Cement ConcreteFederal Highway AdministrationConcrete · Thermal expansion: typical range for portland cement concrete (aggregate dependent)
- 11EOS Titanium Ti64 Grade 23 Material Data SheetEOS GmbHarchived copyDMLS Ti-6Al-4V ELI Titanium · Thermal expansion: mean 25-100 °C, ASTM E228; EOS Ti64 Grade 23 (=ELI) on EOS M 290 40 µm; condition not stated (sheet's mechanical data are heat treated)
- 12Best Practice Guidelines for Structural Fire Resistance Design of Concrete and Steel Buildings (TN 1681)National Institute of Standards and Technologyarchived copyConcrete · Specific heat: typical (NIST guidance for thermal analysis)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS Ti-6Al-4V ELI Titanium is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Which is lighter, Concrete or DMLS Ti-6Al-4V ELI Titanium?
Concrete is lighter: 2,320 kg/m³ against 4,400 kg/m³ for DMLS Ti-6Al-4V ELI Titanium.
Which is stiffer, Concrete or DMLS Ti-6Al-4V ELI Titanium?
DMLS Ti-6Al-4V ELI Titanium is stiffer: Young's modulus 110 GPa against 25.1 GPa for Concrete, so the same part in DMLS Ti-6Al-4V ELI Titanium deflects less under the same load.
Which is lighter for the same job, Concrete or DMLS Ti-6Al-4V ELI Titanium?
For the same stiffness or strength: Concrete is lighter for a stiff panel or plate; DMLS Ti-6Al-4V ELI Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending).
| Part that must be | Concrete | DMLS Ti-6Al-4V ELI Titanium |
|---|---|---|
| Stiff rod or tie (tension) | 2.31x heavier | lighter |
| Stiff beam (bending) | 10% heavier | lighter |
| Stiff panel or plate | lighter | 16% heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Concrete or DMLS Ti-6Al-4V ELI Titanium?
DMLS Ti-6Al-4V ELI Titanium conducts heat better: 6.6 W/m·K against 0.9 W/m·K for Concrete.
Which expands less with temperature?
DMLS Ti-6Al-4V ELI Titanium expands less: 9 µm/m·K against 10 µm/m·K for Concrete.
Related comparisons
- Concrete vs. PCB Board FR-4, 2 copper planes
- Concrete vs. Plastic PTFE
- Concrete vs. Brick
- Concrete vs. PCB Laminate FR-4
- DMLS Ti-6Al-4V ELI Titanium vs. Titanium
- DMLS Ti-6Al-4V ELI Titanium vs. Titanium Ti-6Al-4V
- DMLS Ti-6Al-4V ELI Titanium vs. Stainless Steel 17-4PH
- DMLS Ti-6Al-4V ELI Titanium vs. Steel AISI 4340