Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Sources9 documents: BASF, National Ready Mixed Concrete Association, Federal Highway Administration, Oak Ridge National Laboratory, Covestro, USDA Forest Products Laboratory, National Institute of Standards and Technology
Concrete
Normal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC review
Plastic Nylon PA66
BASF Ultramid A3K (PA66, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)
CIP 36: Structural Lightweight ConcreteNational Ready Mixed Concrete Associationarchived copyConcrete · Density: range for normalweight concrete
5
The Effect of Elevated Temperature on Concrete Materials and Structures: A Literature Review (ORNL/TM-2005/553)Oak Ridge National Laboratoryarchived copyConcrete · Poisson's ratio: general range at normal ambient conditions (overall 0.11-0.32)Concrete · Max service temperature: code long-term temperature limit (ASME Code, concrete containments)
6
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA66 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
Thermal Coefficient of Portland Cement ConcreteFederal Highway AdministrationConcrete · Thermal expansion: typical range for portland cement concrete (aggregate dependent)
9
Best Practice Guidelines for Structural Fire Resistance Design of Concrete and Steel Buildings (TN 1681)National Institute of Standards and Technologyarchived copyConcrete · Specific heat: typical (NIST guidance for thermal analysis)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Which is lighter, Concrete or Plastic Nylon PA66?
Plastic Nylon PA66 is lighter: 1,130 kg/m³ against 2,320 kg/m³ for Concrete.
Which is stiffer, Concrete or Plastic Nylon PA66?
Concrete is stiffer: Young's modulus 25.1 GPa against 3 GPa for Plastic Nylon PA66, so the same part in Concrete deflects less under the same load.
Which is lighter for the same job, Concrete or Plastic Nylon PA66?
For the same stiffness or strength: Concrete is lighter for a stiff rod or tie (tension), stiff beam (bending); Plastic Nylon PA66 is lighter for a stiff panel or plate.
Part that must be
Concrete
Plastic Nylon PA66
Stiff rod or tie (tension)
lighter
4.08x heavier
Stiff beam (bending)
lighter
41% heavier
Stiff panel or plate
1% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which handles higher temperatures, Concrete or Plastic Nylon PA66?
Plastic Nylon PA66 does: 101 °C against 65 °C for Concrete.
Which conducts heat better, Concrete or Plastic Nylon PA66?
Concrete conducts heat better: 0.9 W/m·K against 0.33 W/m·K for Plastic Nylon PA66.
Which expands less with temperature?
Concrete expands less: 10 µm/m·K against 98 µm/m·K for Plastic Nylon PA66.