Materials / Compare

Concrete vs. Plastic Polycarbonate

Compare Concrete vs. Plastic Polycarbonate strength, stiffness, weight and thermal properties.

ConcreteCast
Plastic PolycarbonateBulk polymer (molded or machined)
MechanicalConcretePlastic Polycarbonate
Yield strengthnone (brittle)65MPa1
Ultimate tensile strengthnot sourced65MPa1
Compressive strength27.6MPa2not sourced
Flexural strengthnot sourced97MPa1
Elongation at breaknone (brittle)125%1
Young's modulus (stiffness)design value25.1GPa32.4GPa1
Density2,240–2,400kg/m³41,200kg/m³1
Strength to weightnot sourced54.2kN·m/kg
Stiffness to weight10.8MN·m/kg5.41x higher2MN·m/kg
Poisson's ratio0.15–0.250.386
Shear modulus10.7GPa12.3x stiffer in shear0.87GPa
Bulk modulus12.9GPa3.86x higher3.33GPa
Speed of sound3,289m/s2.33x faster1,414m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30ConcretePlastic Polycarbonate
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Polycarbonate
Strength against densityHigher and further left: stronger for its weight
ThermalConcretePlastic Polycarbonate
Thermal conductivity0.9W/m·K74.5x more heat through a fin0.2W/m·K1
Thermal expansion8–12µm/m·K865µm/m·K1
100 mm part over a 50 °C swing50µm growth6.5x less325µm growth
Specific heat900J/kg·K91,172J/kg·K1030% higher
Heats up and cools (diffusivity)0.431mm²/s3.03x faster0.142mm²/s
Thermal shock resistancenot sourced51.7W/m
Glass transitionnot sourced144°C1
Max service temperature65°C5UL 746B RTI125°C160 °C hotter
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30ConcretePlastic Polycarbonate
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30ConcretePlastic Polycarbonate
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources10 documents: Covestro, National Ready Mixed Concrete Association, Federal Highway Administration, Oak Ridge National Laboratory, USDA Forest Products Laboratory, National Institute of Standards and Technology, Bayer MaterialScience
Concrete
Normal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC review
Plastic Polycarbonate
Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values
  1. 1
    Makrolon 2405 Technical Data SheetCovestroPlastic Polycarbonate · Yield strength: typical, tensile yieldPlastic Polycarbonate · Ultimate tensile strength: typical, stress at breakPlastic Polycarbonate · Flexural strength: typical, flexural strengthPlastic Polycarbonate · Elongation at break: typical, strain at breakPlastic Polycarbonate · Young's modulus (stiffness): typicalPlastic Polycarbonate · Density: typicalPlastic Polycarbonate · Thermal conductivity: typical, through-plane, 23 CPlastic Polycarbonate · Thermal expansion: typical, 23-55 C, parallel and normalPlastic Polycarbonate · Glass transition: typical, DSC 10 C/minPlastic Polycarbonate · Max service temperature: UL 746B RTI, tensile strength, 1.5 mm
  2. 2
    CIP 35: Testing Compressive Strength of ConcreteNational Ready Mixed Concrete Associationarchived copyConcrete · Compressive strength: specified compressive strength class (f'c), not a measured typical
  3. 3
    LRFD Steel Girder Superstructure Bridge Design Example, Design Step 2: Concrete Deck DesignFederal Highway AdministrationConcrete · Young's modulus (stiffness): design value: AASHTO LRFD 5.4.2.4 applied by FHWA to f'c = 4.0 ksi normal-weight concrete
  4. 4
    CIP 36: Structural Lightweight ConcreteNational Ready Mixed Concrete Associationarchived copyConcrete · Density: range for normalweight concrete
  5. 5
    The Effect of Elevated Temperature on Concrete Materials and Structures: A Literature Review (ORNL/TM-2005/553)Oak Ridge National Laboratoryarchived copyConcrete · Poisson's ratio: general range at normal ambient conditions (overall 0.11-0.32)Concrete · Max service temperature: code long-term temperature limit (ASME Code, concrete containments)
  6. 6
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
  7. 7
    Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of WoodUSDA Forest Products LaboratoryConcrete · Thermal conductivity: typical (comparative value)
  8. 8
    Thermal Coefficient of Portland Cement ConcreteFederal Highway AdministrationConcrete · Thermal expansion: typical range for portland cement concrete (aggregate dependent)
  9. 9
    Best Practice Guidelines for Structural Fire Resistance Design of Concrete and Steel Buildings (TN 1681)National Institute of Standards and Technologyarchived copyConcrete · Specific heat: typical (NIST guidance for thermal analysis)
  10. 10
    Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Which is lighter, Concrete or Plastic Polycarbonate?

Plastic Polycarbonate is lighter: 1,200 kg/m³ against 2,320 kg/m³ for Concrete.

Which is stiffer, Concrete or Plastic Polycarbonate?

Concrete is stiffer: Young's modulus 25.1 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Concrete deflects less under the same load.

Which is lighter for the same job, Concrete or Plastic Polycarbonate?

For the same stiffness or strength: Concrete is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beConcretePlastic Polycarbonate
Stiff rod or tie (tension)lighter5.41x heavier
Stiff beam (bending)lighter1.67x heavier
Stiff panel or platelighter13% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which handles higher temperatures, Concrete or Plastic Polycarbonate?

Plastic Polycarbonate does: 125 °C against 65 °C for Concrete.

Which conducts heat better, Concrete or Plastic Polycarbonate?

Concrete conducts heat better: 0.9 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.

Which expands less with temperature?

Concrete expands less: 10 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.