Materials / Compare

Copper C110 vs. Plastic PTFE

Compare Copper C110 vs. Plastic PTFE strength, stiffness, weight and thermal properties.

Copper C110Wrought
Plastic PTFEBulk polymer (molded or machined)
MechanicalCopper C110Plastic PTFE
Yield strength69MPa17.67x stronger9MPa2
Ultimate tensile strength221MPa15.62x stronger39.3MPa3
Elongation at break55%1350%36.36x more ductile
Young's modulus (stiffness)117GPa1not sourced
Density8,913kg/m³12,160kg/m³34.13x lighter
Strength to weight7.74kN·m/kg1.86x higher4.17kN·m/kg
Stiffness to weight13.1MN·m/kgnot sourced
Poisson's ratio0.3440.462
Shear modulus43.7GPanot sourced
Bulk modulus122GPanot sourced
Speed of sound3,626m/snot sourced
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Plastic PTFE
Strength against densityHigher and further left: stronger for its weight
ThermalCopper C110Plastic PTFE
Thermal conductivity391W/m·K11,564x more heat through a fin0.25W/m·K2
Thermal expansion16.9µm/m·K15.92x less100µm/m·K2
100 mm part over a 50 °C swing84.5µm growth5.92x less500µm growth
Specific heat385J/kg·K11,400J/kg·K23.63x higher
Heats up and cools (diffusivity)114mm²/s1,378x faster0.0827mm²/s
Thermal shock resistance8,992W/mnot sourced
Melting pointsolidus-liquidus1,065–1,083°C1second melting peak327°C3
Max service temperaturenot sourcedservice temperature260°C5
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Plastic PTFE
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Plastic PTFE
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Copper Development Association, Chemours, Wieland
Copper C110
C11000 ETP copper, annealed to 0.050 mm grain size (OS050), 1 in. rod, copper.org typical values
Plastic PTFE
Chemours Teflon PTFE 7C X granular molding resin, typical values (tensile/elongation measured on 0.13 mm skived tape)
  1. 1
    C11000 Alloy (copper.org)Copper Development Associationarchived copyCopper C110 · Yield strength: typical, 0.5% extension under loadCopper C110 · Ultimate tensile strength: typicalCopper C110 · Elongation at break: typical, 1 in. rodCopper C110 · Young's modulus (stiffness): typicalCopper C110 · Density: nominalCopper C110 · Thermal conductivity: typical, 20 °CCopper C110 · Thermal expansion: typical, mean 20-100 °CCopper C110 · Specific heat: typical, 20 °CCopper C110 · Melting point: solidus-liquidus
  2. 2
    Teflon PTFE Fluoropolymer Resin Properties HandbookChemoursarchived copyPlastic PTFE · Yield strength: typical yield strength at 23 °C (Teflon PTFE, Table 8)Plastic PTFE · Poisson's ratio: typical, 23 °C (Teflon PTFE resins, Chemours handbook)Plastic PTFE · Thermal conductivity: typical, granular resin, 4.6 mm specimenPlastic PTFE · Thermal expansion: typical, granular resin, 23-60 °C (ASTM E228)Plastic PTFE · Specific heat: typical, granular resin, 20 °C (ASTM D4591)
  3. 3
    Teflon PTFE 7C X Product InformationChemoursarchived copyPlastic PTFE · Ultimate tensile strength: typical, skived tape 0.13 mmPlastic PTFE · Elongation at break: typical, skived tape 0.13 mmPlastic PTFE · Density: typical (standard specific gravity, ASTM D4894)Plastic PTFE · Melting point: second melting peak (sintered polymer), +/-10
  4. 4
    Wieland-K32 (Cu-ETP, C11000) Data SheetWielandarchived copyCopper C110 · Poisson's ratio: reference value at room temperature (Wieland-K32 = Cu-ETP = C11000, rolled products)
  5. 5
    Teflon PTFE 6C X Product InformationChemoursarchived copyPlastic PTFE · Max service temperature: service temperature (Chemours general Teflon PTFE statement)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Copper C110 stronger than Plastic PTFE?

Copper C110 is stronger: its yield strength is 69 MPa against 9 MPa for Plastic PTFE (7.67x).

Which is lighter, Copper C110 or Plastic PTFE?

Plastic PTFE is lighter: 2,160 kg/m³ against 8,913 kg/m³ for Copper C110.

Which is lighter for the same job, Copper C110 or Plastic PTFE?

For the same stiffness or strength: Copper C110 is lighter for a strong rod or tie; Plastic PTFE is lighter for a strong beam, strong panel or plate.

Part that must beCopper C110Plastic PTFE
Strong rod or tielighter1.86x heavier
Strong beam6% heavierlighter
Strong panel or plate49% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Copper C110 or Plastic PTFE?

Plastic PTFE stretches further before it breaks: 350% elongation at break against 55% for Copper C110.

Thermal

Which conducts heat better, Copper C110 or Plastic PTFE?

Copper C110 conducts heat better: 391 W/m·K against 0.25 W/m·K for Plastic PTFE.

Which expands less with temperature?

Copper C110 expands less: 16.9 µm/m·K against 100 µm/m·K for Plastic PTFE.

Related comparisons