Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: EOS GmbH, UltiMaker, Cleveland-Cliffs
DMLS 17-4PH Stainless Steel
EOS StainlessSteel 17-4PH IndustryLine (powder 9011-0041), EOS M 290, 40 µm, default job 17-4PH_040_StainlessM291_100, as built, horizontal; ISO 6892 & ASTM E8M
Plastic TPU
Ultimaker TPU 95A, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 29, 2022.
1
EOS StainlessSteel 17-4PH IndustryLine Material Data Sheet, M 290EOS GmbHarchived copyDMLS 17-4PH Stainless Steel · Yield strength: mean, as built, horizontal (N=72)DMLS 17-4PH Stainless Steel · Ultimate tensile strength: mean, as built, horizontal (N=72)DMLS 17-4PH Stainless Steel · Elongation at break: mean at break, as built, horizontalDMLS 17-4PH Stainless Steel · Density: mean part density (ISO 3369)DMLS 17-4PH Stainless Steel · Thermal expansion: mean 25-100 °C, ASTM E228, AFTER atmospheric heat treatment (as-built value not published)
17-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsDMLS 17-4PH Stainless Steel · Young's modulus (stiffness): base material: wrought 17-4 PH, Condition H 900 (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Poisson's ratio: base material: wrought 17-4 PH, all conditions (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Thermal conductivity: base material: wrought 17-4 PH, Condition H 900, at 149 °C (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Specific heat: base material: wrought 17-4 PH, Condition A, 0-100 °C (Cleveland-Cliffs)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS 17-4PH Stainless Steel and Plastic TPU are 3D printed: their properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS 17-4PH Stainless Steel stronger than Plastic TPU?
DMLS 17-4PH Stainless Steel is stronger: its yield strength is 861 MPa against tensile strength 23.7 MPa for Plastic TPU (36.3x).
Which is lighter, DMLS 17-4PH Stainless Steel or Plastic TPU?
Plastic TPU is lighter: 1,220 kg/m³ against 7,790 kg/m³ for DMLS 17-4PH Stainless Steel.
Which is stiffer, DMLS 17-4PH Stainless Steel or Plastic TPU?
DMLS 17-4PH Stainless Steel is stiffer: Young's modulus 197 GPa against 0.067 GPa for Plastic TPU, so the same part in DMLS 17-4PH Stainless Steel deflects less under the same load.
Which is lighter for the same job, DMLS 17-4PH Stainless Steel or Plastic TPU?
For the same stiffness or strength: DMLS 17-4PH Stainless Steel is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam; Plastic TPU is lighter for a strong panel or plate.
Part that must be
DMLS 17-4PH Stainless Steel
Plastic TPU
Stiff rod or tie (tension)
lighter
460x heavier
Stiff beam (bending)
lighter
8.49x heavier
Stiff panel or plate
lighter
2.24x heavier
Strong rod or tie
lighter
5.69x heavier
Strong beam
lighter
1.72x heavier
Strong panel or plate
6% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).