Mechanical
Yield strength861MPasourcemean, as built, horizontal (N=72)372MPasourceproducer-stated, cold drawn
Ultimate tensile strength886MPasourcemean, as built, horizontal (N=72)441MPasourceproducer-stated, cold drawn
Elongation at break19.9%sourcemean at break, as built, horizontal15%sourcein 2 in (50.8 mm)
Young's modulus (stiffness)197GPasourcebase material: wrought 17-4 PH, Condition H 900 (Cleveland-Cliffs)200GPasourcebase material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
Density7,790kg/m³sourcemean part density (ISO 3369)7,861kg/m³sourcebase material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
Strength to weight110kN·m/kg2.33x higher47.3kN·m/kg
Stiffness to weight25.3MN·m/kg25.4MN·m/kg
Poisson's ratio0.272sourcebase material: wrought 17-4 PH, all conditions (Cleveland-Cliffs)0.32sourcebase material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
Shear modulus77.4GPa2% stiffer in shear75.7GPa
Bulk modulus144GPa185GPa
Speed of sound5,029m/s5,043m/s
Thermal
Thermal conductivity17.9W/m·Ksourcebase material: wrought 17-4 PH, Condition H 900, at 149 °C (Cleveland-Cliffs)51.9W/m·Ksourcebase material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
Thermal expansion10.4µm/m·Ksourcemean 25-100 °C, ASTM E228, AFTER atmospheric heat treatment (as-built value not published)12µm/m·Ksourcebase material: unalloyed carbon steel, Ovako family table (S275JR, 'none alloyed structural steels', C <= 0.21%); mean 20-300 °C
100 mm part over a 50 °C swing52µm growth15% less60µm growth
Specific heat460J/kg·Ksourcebase material: wrought 17-4 PH, Condition A, 0-100 °C (Cleveland-Cliffs)486J/kg·Ksourcebase material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
Heats up and cools (diffusivity)5mm²/s13.6mm²/s2.72x faster
Thermal shock resistance5,474W/m5,473W/m
Values forEOS StainlessSteel 17-4PH IndustryLine (powder 9011-0041), EOS M 290, 40 µm, default job 17-4PH_040_StainlessM291_100, as built, horizontal; ISO 6892 & ASTM E8MAISI 1018 cold drawn bar (Niagara LaSalle, cold-finished bar producer)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS 17-4PH Stainless Steel is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is DMLS 17-4PH Stainless Steel stronger than Steel AISI 1018?

DMLS 17-4PH Stainless Steel is stronger: its yield strength is 861 MPa against 372 MPa for Steel AISI 1018 (2.31x).

Which is lighter, DMLS 17-4PH Stainless Steel or Steel AISI 1018?

DMLS 17-4PH Stainless Steel is lighter: 7,790 kg/m³ against 7,861 kg/m³ for Steel AISI 1018.

Which is stiffer, DMLS 17-4PH Stainless Steel or Steel AISI 1018?

Steel AISI 1018 is stiffer: Young's modulus 200 GPa against 197 GPa for DMLS 17-4PH Stainless Steel, so the same part in Steel AISI 1018 deflects less under the same load.

Which is lighter for the same job, DMLS 17-4PH Stainless Steel or Steel AISI 1018?

For the same stiffness or strength: DMLS 17-4PH Stainless Steel is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beDMLS 17-4PH Stainless SteelSteel AISI 1018
Stiff rod or tie (tension)about equalabout equal
Stiff beam (bending)about equalabout equal
Stiff panel or plateabout equalabout equal
Strong rod or tielighter2.33x heavier
Strong beamlighter1.77x heavier
Strong panel or platelighter1.53x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, DMLS 17-4PH Stainless Steel or Steel AISI 1018?

Steel AISI 1018 conducts heat better: 51.9 W/m·K against 17.9 W/m·K for DMLS 17-4PH Stainless Steel.

Which expands less with temperature?

DMLS 17-4PH Stainless Steel expands less: 10.4 µm/m·K against 12 µm/m·K for Steel AISI 1018.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumStainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS 17-4PH Stainless SteelSteel AISI 1018
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumStainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30DMLS 17-4PH Stainless SteelSteel AISI 1018
Strength against density

Related comparisons