Materials / Compare

Drywall vs. Plastic Nylon PA6

Compare Drywall vs. Plastic Nylon PA6 strength, stiffness, weight and thermal properties.

Change either side
DrywallNatural
Plastic Nylon PA6Bulk polymer (molded or machined)
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)90MPasourcetypical, dry
Ultimate tensile strength1–2MPasourceambient range reported in review (Australian studies)not sourced
Compressive strength2.4MPasourcetypical, 70 F / 50% RHnot sourced
Elongation at breaknot sourced10%sourcenominal strain at break, dry
Young's modulus (stiffness)1–2GPasourceambient range reported in review (Australian studies)3.5GPasourcetypical, dry
Densitynot sourced1,130kg/m³sourcetypical
Strength to weightnot sourced79.6kN·m/kg
Stiffness to weightnot sourced3.1MN·m/kg
Poisson's rationot sourced0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
Shear modulusnot sourced1.25GPa
Bulk modulusnot sourced5.83GPa
Speed of soundnot sourced1,760m/s
Thermal
Thermal conductivitynot sourced0.33W/m·Ksourcetypical
Thermal expansion16.7µm/m·Ksourcetypical, unrestrained, 3.3-32 C102µm/m·Ksourcelongitudinal, 23-55 °C
100 mm part over a 50 °C swing83.5µm growth6.11x less510µm growth
Specific heat1,090J/kg·Ksourcetypical (from ASHRAE Handbook of Fundamentals, per GA)1,700J/kg·Ksourcetypical
Heats up and cools (diffusivity)not sourced0.172mm²/s
Thermal shock resistancenot sourced49.9W/m
Melting pointnot sourced220°CsourceDSC
Max service temperature52°Csourcemanufacturer sustained-exposure limit87°CsourceIEC 60216 temperature index, 20000 h
Values for1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittalBASF Ultramid B3S (PA6, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Drywall stronger than Plastic Nylon PA6?

Plastic Nylon PA6 is stronger: its yield strength is 90 MPa against tensile strength 1.5 MPa for Drywall (60x).

Which is stiffer, Drywall or Plastic Nylon PA6?

Plastic Nylon PA6 is stiffer: Young's modulus 3.5 GPa against 1.5 GPa for Drywall, so the same part in Plastic Nylon PA6 deflects less under the same load.

Which expands less with temperature?

Drywall expands less: 16.7 µm/m·K against 102 µm/m·K for Plastic Nylon PA6.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Nylon PA6
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Nylon PA6
Strength against density

Related comparisons