Materials / Compare

Drywall vs. Plastic PETG

Compare Drywall vs. Plastic PETG strength, stiffness, weight and thermal properties.

Change either side
DrywallNatural
Plastic PETG3D printed (FDM)
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)46.2MPasourcetypical
Ultimate tensile strength1–2MPasourceambient range reported in review (Australian studies)46.2MPasourcetypical, peak stress (= stress at yield)
Compressive strength2.4MPasourcetypical, 70 F / 50% RHnot sourced
Flexural strengthnot sourced78.9MPasourcetypical
Elongation at breaknot sourced7.6%sourcetypical
Young's modulus (stiffness)1–2GPasourceambient range reported in review (Australian studies)1.94GPasourcetypical
Densitynot sourced1,270kg/m³sourcetypical
Strength to weightnot sourced36.4kN·m/kg
Stiffness to weightnot sourced1.53MN·m/kg
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourced1,236m/s
Thermal
Thermal conductivitynot sourced0.21W/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical
Thermal expansion16.7µm/m·Ksourcetypical, unrestrained, 3.3-32 C51µm/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical
100 mm part over a 50 °C swing83.5µm growth3.05x less255µm growth
Specific heat1,090J/kg·Ksourcetypical (from ASHRAE Handbook of Fundamentals, per GA)1,300J/kg·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)
Heats up and cools (diffusivity)not sourced0.127mm²/s
Thermal shock resistancenot sourcednot sourced
Glass transitionnot sourced77.4°Csourcetypical
Max service temperature52°Csourcemanufacturer sustained-exposure limit76.2°CsourceHDT 0.455 MPa (printed specimens)
Values for1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittalUltimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Drywall stronger than Plastic PETG?

Plastic PETG is stronger: its yield strength is 46.2 MPa against tensile strength 1.5 MPa for Drywall (30.8x).

Which is stiffer, Drywall or Plastic PETG?

Plastic PETG is stiffer: Young's modulus 1.94 GPa against 1.5 GPa for Drywall, so the same part in Plastic PETG deflects less under the same load.

Which expands less with temperature?

Drywall expands less: 16.7 µm/m·K against 51 µm/m·K for Plastic PETG.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PETG
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PETG
Strength against density

Related comparisons