Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittal
Plastic LCP GF30
Sumitomo Chemical SUMIKASUPER LCP E6006L (30% glass fibre; high strength, low shrinkage); SUMIKASUPER LCP Technical Note, Version 04 / Nov. 2023, typical values.
1
Mechanical Properties of Gypsum Board at Elevated TemperaturesUSDA Forest Products LaboratoryDrywall · Ultimate tensile strength: ambient range reported in review (Australian studies)Drywall · Young's modulus (stiffness): ambient range reported in review (Australian studies)
2
SUMIKASUPER LCP Technical Note, Version 04 (2023)Sumitomo Chemicalarchived copyPlastic LCP GF30 · Ultimate tensile strength: tensile strength (ISO 527)Plastic LCP GF30 · Flexural strength: typical (ISO 178)Plastic LCP GF30 · Elongation at break: tensile elongation (ISO 527)Plastic LCP GF30 · Young's modulus (stiffness): tensile modulus (ISO 527)Plastic LCP GF30 · Density: typicalPlastic LCP GF30 · Thermal conductivity: hot disk (ISO 22007-2), temperature not statedPlastic LCP GF30 · Thermal expansion: flow direction (MD), mean 50-150 °CPlastic LCP GF30 · Specific heat: ASTM E1269, temperature not statedPlastic LCP GF30 · Max service temperature: HDT 1.8 MPa (ISO 75)
3
GA-235-2023 Gypsum Board Typical Mechanical and Physical PropertiesGypsum AssociationDrywall · Compressive strength: typical, 70 F / 50% RHDrywall · Thermal expansion: typical, unrestrained, 3.3-32 CDrywall · Specific heat: typical (from ASHRAE Handbook of Fundamentals, per GA)
4
Sheetrock Brand UltraLight Panels Submittal Sheet (WB2501)USGarchived copyDrywall · Max service temperature: manufacturer sustained-exposure limit
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Drywall stronger than Plastic LCP GF30?
Plastic LCP GF30 is stronger: its tensile strength is 115 MPa against 1.5 MPa for Drywall (76.7x).
Which is stiffer, Drywall or Plastic LCP GF30?
Plastic LCP GF30 is stiffer: Young's modulus 11.5 GPa against 1.5 GPa for Drywall, so the same part in Plastic LCP GF30 deflects less under the same load.
Thermal
Which expands less with temperature?
Drywall expands less: 16.7 µm/m·K against 20 µm/m·K for Plastic LCP GF30.