Materials / Compare

Drywall vs. SLA Resin Standard

Compare Drywall vs. SLA Resin Standard strength, stiffness, weight and thermal properties.

Change either side
DrywallNatural
SLA Resin Standard3D printed (SLA resin)
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength1–2MPasourceambient range reported in review (Australian studies)60MPasourcetypical
Compressive strength2.4MPasourcetypical, 70 F / 50% RHnot sourced
Flexural strengthnot sourced105MPasourcetypical
Elongation at breaknot sourced8%sourcetypical
Young's modulus (stiffness)1–2GPasourceambient range reported in review (Australian studies)2.75GPasourcetypical
Densitynot sourcednot sourced
Strength to weightnot sourcednot sourced
Stiffness to weightnot sourcednot sourced
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourcednot sourced
Thermal
Thermal conductivitynot sourcednot sourced
Thermal expansion16.7µm/m·Ksourcetypical, unrestrained, 3.3-32 Cnot sourced
100 mm part over a 50 °C swing83.5µm growthnot sourced
Specific heat1,090J/kg·Ksourcetypical (from ASHRAE Handbook of Fundamentals, per GA)not sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistancenot sourcednot sourced
Max service temperature52°Csourcemanufacturer sustained-exposure limit59°CsourceHDT 1.8 MPa
Values for1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittalFormlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Drywall stronger than SLA Resin Standard?

SLA Resin Standard is stronger: its tensile strength is 60 MPa against 1.5 MPa for Drywall (40x).

Which is stiffer, Drywall or SLA Resin Standard?

SLA Resin Standard is stiffer: Young's modulus 2.75 GPa against 1.5 GPa for Drywall, so the same part in SLA Resin Standard deflects less under the same load.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless Steel
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrick
Strength against density

Related comparisons