Materials / Compare

Drywall vs. Steel A992

Compare Drywall vs. Steel A992 strength, stiffness, weight and thermal properties.

DrywallNatural
Steel A992Wrought
MechanicalDrywallSteel A992
Yield strengthnot given (tensile used)385MPa1
Ultimate tensile strength1–2MPa2505MPa1
Compressive strength2.4MPa3not sourced
Elongation at breaknot sourced24.2%1
Young's modulus (stiffness)1–2GPa2design value200GPa4
Densitynot sourced7,850kg/m³5
Strength to weightnot sourced49kN·m/kg
Stiffness to weightnot sourced25.5MN·m/kg
Poisson's rationot sourceddesign value0.34
Shear modulusnot sourced76.9GPa
Bulk modulusnot sourced167GPa
Speed of soundnot sourced5,048m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Steel A992
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Steel A992
Strength against densityHigher and further left: stronger for its weight
ThermalDrywallSteel A992
Thermal conductivitynot sourced48W/m·K5
Thermal expansion16.7µm/m·K312µm/m·K539% less
100 mm part over a 50 °C swing83.5µm growth60µm growth39% less
Specific heat1,090J/kg·K3base material460–480J/kg·K6
Heats up and cools (diffusivity)not sourced13mm²/s
Thermal shock resistancenot sourced5,390W/m
Max service temperature52°C7not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Steel A992
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Steel A992
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources7 documents: American Institute of Steel Construction, USDA Forest Products Laboratory, Gypsum Association, bauforumstahl (ArcelorMittal), Ovako, USG
Drywall
1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittal
Steel A992
ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
  1. 1
    Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel A992 · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel A992 · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel A992 · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
  2. 2
    Mechanical Properties of Gypsum Board at Elevated TemperaturesUSDA Forest Products LaboratoryDrywall · Ultimate tensile strength: ambient range reported in review (Australian studies)Drywall · Young's modulus (stiffness): ambient range reported in review (Australian studies)
  3. 3
    GA-235-2023 Gypsum Board Typical Mechanical and Physical PropertiesGypsum AssociationDrywall · Compressive strength: typical, 70 F / 50% RHDrywall · Thermal expansion: typical, unrestrained, 3.3-32 CDrywall · Specific heat: typical (from ASHRAE Handbook of Fundamentals, per GA)
  4. 4
    ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel A992 · Young's modulus (stiffness): design value (AISC 360-16)Steel A992 · Poisson's ratio: design value (AISC 360-16 Commentary)
  5. 5
    Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel A992 · Density: nominal (constructional data)Steel A992 · Thermal conductivity: nominal at 20 °CSteel A992 · Thermal expansion: nominal (constructional data, no temperature range stated)
  6. 6
    S275JR Steel GradeOvakoSteel A992 · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
  7. 7
    Sheetrock Brand UltraLight Panels Submittal Sheet (WB2501)USGarchived copyDrywall · Max service temperature: manufacturer sustained-exposure limit

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Drywall stronger than Steel A992?

Steel A992 is stronger: its yield strength is 385 MPa against tensile strength 1.5 MPa for Drywall (257x).

Which is stiffer, Drywall or Steel A992?

Steel A992 is stiffer: Young's modulus 200 GPa against 1.5 GPa for Drywall, so the same part in Steel A992 deflects less under the same load.

Thermal

Which expands less with temperature?

Steel A992 expands less: 12 µm/m·K against 16.7 µm/m·K for Drywall.

Related comparisons